We did not do any mechanical testing (we strictly went with the final result). We did do ICT, JTAG, functional test and microsectioning however, to ensure that there were no cracks present that may cause latent defects. so I do not have exact values to answer your question. Application and cure can be/are controlled as critical variables giving us consistent results in production.
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Friday, June 12, 2009 8:08 AM
To: [log in to unmask]; Kane, Amol (349)
Subject: RE: [TN] Corner ball pad cratering
How can you predict/measure the added strength the corner BGA bonding is
providing. Application/curing are critical elements.
Victor,
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
Sent: Friday, June 12, 2009 7:03 AM
To: [log in to unmask]
Subject: Re: [TN] Corner ball pad cratering
Genny,
We have experienced a very similar phenomenon on one of our product
boards. The BGA was 1.3" square, and there was pad cratering along the
corner pads. The laminate was a high Tg, with added filler to minimize
Z-axis CTE. Chaning the laminate was not an option, so we had to come up
with a process solution to the problem. We determined that the cratering
was not occurring during reflow cool down (but was later, at a
indeterminate process step during board assembly). We did a simple set
of expts with 3 random replications of each:
1. corner bonding prior to reflow (chipbonder 3609)
2. corner bonding immediately after reflow
3. using a SMT pallet throuout the process (so as to eliminate handling
stresses)
We made sure that at least 1/4th length of each BGA side was covered by
the bonding material. In all 3 cases we could manufacture 100% defect
free product. Then based on the simplicity, corner bonding after reflow
was instituted as the preferred stress mitigation technique.
Might be worth a shot to do something similar.
Regards,
Amol
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Thursday, June 11, 2009 4:10 PM
To: [log in to unmask]
Subject: [TN] Corner ball pad cratering
Hello all,
If you have identified a BGA with corner ball pad cratering, what would
be your suggestions to correct this condition?
Our thoughts:
1. We plan to evaluate our handling processes to reduce/remove
excessive flex/strain occurring around this part
2. We plan to evaluate corner bonding or underfilling for the BGA.
Which do you feel would be the best direction to go? Do you have other
suggestions?
Thanks in advance for all your help
Genny
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
WARNING: Export Control
This document may contain technical data within the definition of the
International Traffic in Arms Regulations (ITAR), and subject to the
Export
Control Laws of the U.S. Government. Transfer of such data by any means
to a
foreign person, whether in the United States or abroad, without proper
export
authorization or other approval from the U.S. Department of State is
prohibited.
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
WARNING: Export Control
This document may contain technical data within the definition of the
International Traffic in Arms Regulations (ITAR), and subject to the Export
Control Laws of the U.S. Government. Transfer of such data by any means to a
foreign person, whether in the United States or abroad, without proper export
authorization or other approval from the U.S. Department of State is
prohibited.
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|