TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Randall L Bock <[log in to unmask]>
Date:
Thu, 4 Jun 2009 11:43:15 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
From:
Bev Christian <[log in to unmask]>
content-transfer-encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (229 lines)
Randy,
We are talking about non-conductive and hopefully (!) non-corrosive
organic underfills.
Bev
RIM

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Randall L Bock
Sent: Thursday, June 04, 2009 11:33 AM
To: [log in to unmask]
Subject: Re: [TN] Underfill Workmanship Pass/fail Criteria Proposal

By material is this solder or someother substance??  Solder could pose a
short issue if it came loose.  Other material could also pose the same
concern. 


Randy Bock  Sr.
Quality Engineer / Product Quality Manager
Enterprise Quality Assurance
(Email) [log in to unmask]
Newtown Building 2
203 270-4931  (NT2)
8-426-4931
(Fax)203-270-4982
Shelton 27 WV  203-922-4014
(Cell) 203 300-3547


Pitney Bowes "Engineering the Flow of Communication"

This email message may contain confidential, proprietary and /or
privileged information. It is intended only for the use of the intended
recipient(s).  If you receive this in error, please immediately advise
the sender by reply email and delete this email message.  Any
disclosure, copying, distribution or use of the information contained in
this email to or by anyone other than the intended recipient is strictly
prohibited.  Any views expressed in this message are those of the
individual sender, except when the sender specifically states them to be
the views of the company.  Thank You.




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Thursday, June 04, 2009 11:30 AM
To: [log in to unmask]
Subject: Re: [TN] Underfill Workmanship Pass/fail Criteria Proposal

Graham,
No clue.  This is what my Class 3 buddy wanted to see in the proposed
doc.  Anyone want to explain why or refute its inclusion with data?
Bev

-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]] 
Sent: Thursday, June 04, 2009 11:27 AM
To: TechNet E-Mail Forum; Bev Christian
Subject: RE: [TN] Underfill Workmanship Pass/fail Criteria Proposal

Hi Bev
Why would material on the component top be considered a defect?  Process
indicator I can see, but does it impact reliability?

regards,
 - Graham

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Thursday, June 04, 2009 12:07 PM
To: [log in to unmask]
Subject: [TN] Underfill Workmanship Pass/fail Criteria Proposal

TechNetters,
OK after speaking to a couple of industry friends, this is what we have
come up with. I will leave it to them to speak up and identify
themselves, if they wish.  I have written this up in IPC-A-610 format
and have tried to cover all situations for Class 2 and 3 products in
particular.  

If we can nail this, I would like to present this to the IPC as the
first IPC draft doc essentially hammered out by out TechNet community.

Comments readily accepted!
Bev
RIM


Workmanship Standards for BGA and CSP Underfills

Target - Class 1,2,3
*	Component requiring underfill completely underfilled with a good
fillet all the way around, the fillet just approaching the maximum
component body height, completely cured, no encroachment onto other
components and no voiding whatsoever

Acceptable - Class 3
*	At least 50% fillet height up the side of the component body

*	Small pin holes and voids are permissible provided they do not
exceed 5% of fillet surface area and have a maximum diameter of 0.5 mm
(0.020 inches).

Acceptable - Class 1,2
*	Component requiring underfill underfilled such that all balls
are covered, but no evidence of an exterior fillet, no encroachment onto
other components and no voiding whatsoever

*	Component requiring underfill underfilled such that all balls
are covered, with or without an exterior fillet, no encroachment onto
other components and only small voids, not touching any solder joints

*	Component requiring underfill underfilled such that all balls
are covered, with or without an exterior fillet, no encroachment onto
other components and even large voiding, but not touching any solder
joints

*	A void or voids less than or equal to 50% around the perimeter
of one or more solder joints

Defect - Class 1,2,3
*	Underfill completely missing from components where it is
required

*	Underfill not completely covering all the peripheral solder
joints

*	Voiding such that a void traverses the distance between two or
more solder joints under the array device requiring underfill

*	A void or voids more than 50% around the perimeter of one or
more solder joints

*	Material extending on to the top of the BGA or CSP

*	Uncured material

Special Conditions - Class 1,2
*	Encroachment onto other components, but meeting all other
criteria above for target or acceptable conditions will be dealt with as
a pass/fail on a case-by-case basis

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute
non-public information. Any use of this information by anyone other than
the intended recipient is prohibited. If you have received this
transmission in error, please immediately reply to the sender and delete
this information from your system. Use, dissemination, distribution, or
reproduction of this transmission by unintended recipients is not
authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2