TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 4 Jun 2009 07:21:03 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (300 lines)
I agree with you; planes, like automobiles and just about everything
else, have no clear pedigree anymore.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: Thursday, June 04, 2009 4:50 AM
To: [log in to unmask]
Subject: Re: [TN] Test

I also take "pride" if that's the word in my own place. So when I see RR
on
the engines of any plane I'm pleased. I also note that the wings of
Airbus -
and many other planes - are designed and built in UK. Also large part of
avionics, undercarriages and stuff. So wings, avionics, engines, what
else
is there? Actually there is so much work sharing/offsetting to get
customer
contracts these days that I think you would be hard put to say that a
Boeing
or Airbus comes from anywhere in particular. For example recently Boeing
successfully lobbied a major US defence contract for Air refuelling be
cancelled because it went to Airbus/EADS and therefore abroad, not
patriotic, national security, etc. In fact higher proportion of the work
would have been done in US than in Boeing's proposal (just not by
Boeing).


Regards
 
 
Mike




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Wednesday, June 03, 2009 11:38 PM
To: [log in to unmask]
Subject: Re: [TN] Test

:-)
 
 
In a message dated 6/3/2009 2:26:44 P.M. Pacific Daylight Time,  
[log in to unmask] writes:

"If it's  not Boeing. I'm not going."

Of course I grew up in the Pacific NW so  must admit that's mostly a 
regional pride thing.  :-)


At  02:10 PM 6/3/2009, Joe Fjelstad wrote:
>Hi Bob,
>
>I recall  several folks making such comments over time on this forum
an
>elsewhere. I have personally attempted refrained from making  sweeping
>statements but I know folks out there with very strong   opinions. I 
>like flying on
>Boeing planes because I once worked  for  Boeing and know the quality
of 
the
>plane and the evaluation  systems (in general)  but I fly Airbus when
that 
is
>the equipment  being used knowing that I am not  going to live forever,
nor
>am I  going to live in blind  fear either.
>
>I note that Doug  added a comment that is important. The military and
>aerospace are  exempt but the suppliers of the component they use are
not  
 and
>they are not interested in carrying two inventories for part  numbers.
>
>There has been much discussion about the compatibility  (or lack
thereof)
>of tin-lead and lead-free. Werner has mentioned  how trying  to solve
the
>problem by reballing may well be taking  reliability in  the opposite 
>direction
>due to the  additional high temperature thermal  cycles. And tin
whiskers? 
 I
>note that there are new conferences that are  focusing on this  topic.
The
>list goes on...
>
>It is a thorny problem that  seems not to have any clean resolution,
save,
>perhaps, a return to the  sanity of science based decision making
relative 
to
>  electronics  manufacturing rather than hasty emotional,  poorly
thought  
out
>reasons from self serving politicians.
>
>So it  goes...
>
>Best wishes
>Joe
>
>
>In a  message dated 6/3/2009 10:56:34 A.M. Pacific Daylight  Time,
>[log in to unmask] writes:
>
>Joe,   several years ago, at PCB West, I attended a session which I
>believe  was a  panel discussion on RoHS topics.  A comment was made
at
>that time  about the new Airbus being certified as lead-free  and one
of
>the panel  members made the observation that as long as  that was the
>case, he'd never  get on board an Airbus.  You  were on that panel, and
I
>was just  curious if you remember  that.
>
>
>Bob
>
>-----Original   Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of  Joe  Fjelstad
>Sent: Wednesday, June 03, 2009 12:38  PM
>To:  [log in to unmask]
>Subject: Re: [TN]  Test
>
>Thanks Steve
>
>
>This  was both  sad  event and very sobering.
>
>
>I recall hearing a  few  years back of data being presented  indicating
>that  shock and  vibration resistance goes down for lead-free  solders
>over time with use.
>
>Has this been repeated,  verified or seen by anyone  else?
>
>Joe
>
>
>**************Shop Inspiron,  Studio and XPS Laptops at   Dell.com
>(http://pr.atwola.com/promoclk/100126575x1222616459x1201464730/aol?redi
r
>=http:%2F%2Fad.d
>oubleclick.net%2Fclk%3B215218145%3B37264238%3Bd)
>
>---------------------------------------------------
>Technet   Mail List provided as a service by IPC using LISTSERV 15.0
To
>unsubscribe,  send a message to [log in to unmask] with following  text
in
>the BODY (NOT the  subject field): SIGNOFF Technet To  temporarily halt
or
>(re-start) delivery  of Technet send e-mail to  [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To  receive ONE  mailing per day of all the
>posts: send e-mail to   [log in to unmask]: SET Technet Digest Search the
>archives of previous  posts  at: http://listserv.ipc.org/archives
Please
>visit IPC web  site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
>additional  information, or contact Keach Sasamori at  [log in to unmask]
or
>847-615-7100   ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet   Mail List provided as a service by IPC using LISTSERV 15.0
>To  unsubscribe,  send a message to [log in to unmask] with following
text  
in
>the BODY (NOT the  subject field): SIGNOFF Technet
>To  temporarily halt or (re-start) delivery  of Technet send e-mail  to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To   receive ONE mailing per day of all the posts: send e-mail  to
>[log in to unmask]:  SET Technet Digest
>Search the  archives of previous posts at:   
http://listserv.ipc.org/archives
>Please visit IPC web site   
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional  information,  or contact Keach Sasamori at
[log in to unmask]  
or
>847-615-7100   ext.2815
>-----------------------------------------------------
>
>**************Shop  Inspiron, Studio and XPS Laptops at  Dell.com
>(http://pr.atwola.com/promoclk/100126575x1222616459x1201464730/aol?redi
r=ht
tp:%2F%2Fad.d
>oubleclick.net%2Fclk%3B215218145%3B37264238%3Bd)
>
>---------------------------------------------------
>Technet  Mail List provided as a service by IPC using LISTSERV 15.0
>To  unsubscribe, send a message to [log in to unmask] with following text
in
>the BODY (NOT the subject field): SIGNOFF Technet
>To  temporarily halt or (re-start) delivery of Technet send e-mail to  
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE  mailing per day of all the posts: send e-mail to 
>[log in to unmask]: SET  Technet Digest
>Search the archives of previous posts at:
http://listserv.ipc.org/archives
>Please visit IPC web site  
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional  
>information, or contact Keach Sasamori at [log in to unmask] or  
>847-615-7100  ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet  Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe,  send a message to [log in to unmask] with following text
in
the BODY (NOT the  subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery  of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To  receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]:  SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information,  or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100  ext.2815
-----------------------------------------------------


**************Shop Inspiron, Studio and XPS Laptops at Dell.com 
(http://pr.atwola.com/promoclk/100126575x1222616459x1201464730/aol?redir
=htt
p:%2F%2Fad.d
oubleclick.net%2Fclk%3B215218145%3B37264238%3Bd)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------


***This email, its content, and any files transmitted with it, are
intended solely for the addressee(s) and may be legally privileged
and/or confidential. If you are not the intended recipient, please
contact the sender by return and delete the material from any computer.
Any review, retransmission, dissemination, or other use of, or taking of
any action in reliance upon this information by persons or entities
other than the intended recipient is prohibited.

Messages sent via this medium may be subjected to delays, non-delivery,
and unauthorized alteration. This email has been prepared using
information believed by the author to be reliable and accurate, but
Indium Corporation makes no warranty as to accuracy or completeness.
Indium Corporation does not accept responsibility for changes made to
this email after is was sent. Any opinions or recommendations expressed
herein are solely those of the author. They may be subject to change
without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2