TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Wed, 3 Jun 2009 14:25:26 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dwight Mattix <[log in to unmask]>
Subject:
From:
Dwight Mattix <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"; format=flowed
Parts/Attachments:
text/plain (136 lines)
"If it's not Boeing. I'm not going."

Of course I grew up in the Pacific NW so must admit that's mostly a 
regional pride thing.  :-)


At 02:10 PM 6/3/2009, Joe Fjelstad wrote:
>Hi Bob,
>
>I recall several folks making such comments over time on this forum an
>elsewhere. I have personally attempted refrained from making sweeping
>statements but I know folks out there with very strong  opinions. I 
>like flying on
>Boeing planes because I once worked for  Boeing and know the quality of the
>plane and the evaluation systems (in general)  but I fly Airbus when that is
>the equipment being used knowing that I am not  going to live forever, nor
>am I going to live in blind  fear either.
>
>I note that Doug added a comment that is important. The military and
>aerospace are exempt but the suppliers of the component they use are not  and
>they are not interested in carrying two inventories for part numbers.
>
>There has been much discussion about the compatibility (or lack  thereof)
>of tin-lead and lead-free. Werner has mentioned how trying  to solve the
>problem by reballing may well be taking reliability in  the opposite 
>direction
>due to the additional high temperature thermal  cycles. And tin whiskers? I
>note that there are new conferences that are  focusing on this topic. The
>list goes on...
>
>It is a thorny problem that seems not to have any clean resolution, save,
>perhaps, a return to the sanity of science based decision making relative to
>  electronics manufacturing rather than hasty emotional,  poorly thought out
>reasons from self serving politicians.
>
>So it goes...
>
>Best wishes
>Joe
>
>
>In a message dated 6/3/2009 10:56:34 A.M. Pacific Daylight Time,
>[log in to unmask] writes:
>
>Joe,  several years ago, at PCB West, I attended a session which I
>believe was a  panel discussion on RoHS topics.  A comment was made at
>that time  about the new Airbus being certified as lead-free and one of
>the panel  members made the observation that as long as that was the
>case, he'd never  get on board an Airbus.  You were on that panel, and I
>was just  curious if you remember that.
>
>
>Bob
>
>-----Original  Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe  Fjelstad
>Sent: Wednesday, June 03, 2009 12:38 PM
>To:  [log in to unmask]
>Subject: Re: [TN] Test
>
>Thanks Steve
>
>
>This  was both sad  event and very sobering.
>
>
>I recall hearing a few  years back of data being presented  indicating
>that shock and  vibration resistance goes down for lead-free solders
>over time with use.
>
>Has this been repeated, verified or seen by anyone else?
>
>Joe
>
>
>**************Shop Inspiron, Studio and XPS Laptops at  Dell.com
>(http://pr.atwola.com/promoclk/100126575x1222616459x1201464730/aol?redir
>=http:%2F%2Fad.d
>oubleclick.net%2Fclk%3B215218145%3B37264238%3Bd)
>
>---------------------------------------------------
>Technet  Mail List provided as a service by IPC using LISTSERV 15.0 To
>unsubscribe,  send a message to [log in to unmask] with following text in
>the BODY (NOT the  subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery  of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To  receive ONE mailing per day of all the
>posts: send e-mail to  [log in to unmask]: SET Technet Digest Search the
>archives of previous posts  at: http://listserv.ipc.org/archives Please
>visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>additional  information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100  ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet  Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe,  send a message to [log in to unmask] with following text in
>the BODY (NOT the  subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery  of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To  receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]:  SET Technet Digest
>Search the archives of previous posts at:  http://listserv.ipc.org/archives
>Please visit IPC web site  http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information,  or contact Keach Sasamori at [log in to unmask] or
>847-615-7100  ext.2815
>-----------------------------------------------------
>
>**************Shop Inspiron, Studio and XPS Laptops at Dell.com
>(http://pr.atwola.com/promoclk/100126575x1222616459x1201464730/aol?redir=http:%2F%2Fad.d
>oubleclick.net%2Fclk%3B215218145%3B37264238%3Bd)
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to 
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to 
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site 
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
>information, or contact Keach Sasamori at [log in to unmask] or 
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2