Hi Al,
How to you relate strain measured on the package to the strain in the solder joints? What do you mean be "saturated state cycle"?
The strain range is only a adequate measure under some circumstances, but not all—in others you also need the stress range.
I suggest you follow the procedures in IPC-D-279.
Werner
-----Original Message-----
From: al shirazi <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, Jun 19, 2009 11:38 am
Subject: [TN]
Dear TechNeters,
I am measuring strain of a corner joint of a lead-free Lidless FC-PBGA
package.For the purpose of looking into the fatigue life of the joints under
thermal cycling (ATC profile).
Is recording strain for one cycle after cycling the package for some cycles is
good enough to be referred as the saturated state cycle?After how many cycles
maybe for this type of the package?Any previous experience?
I appreciate your inputs from either experimental point of view or modeling,
Thanks
Al
__________________________________________________________________
Yahoo! Canada Toolbar: Search from anywhere on the web, and bookmark your
favourite sites. Download it now
http://ca.toolbar.yahoo.com.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: S
ET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|