Bill,
I'm going to make the following assumptions and hope that I don't get
pulverized:
What surface finish? HASL - Hot Air Soldered Level (Tin Lead)
What board type? FR-4
It sounds like to me that the boards were stored long enough to get a
level of oxide on them which prevented them from being soldered. In a
prior life, I had operators "clean" boards with a #2 eraser which
removed any oxides prior to soldering. Your customer's "scrubbing"
action may be doing the same thing.
Hope this helps - Good Luck
Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bill Dworak
Sent: Monday, June 15, 2009 1:48 PM
To: [log in to unmask]
Subject: [TN] HAL-Leaded assembly
Hello everybody, I am looking for some knowledge on what I see is a
basic type problem that is driving me crazy. I am a sales guy who covers
a sizable territory and in that territory for a PCB manufacturer (yes
one of those) I have one account that I have been working with for about
4 years now that continuously has issues assembling both hand assembly
as well as pick & place.
The surface finish is HAL (leaded) this is a military account that is
pretty well structured in their processes. What I get told is that there
seems like a contamination is on the surface when they scrub the surface
it makes it better but not 100% better.They have sent back samples for
us to look at , we saw nothing on the surface no contamination nothing
wrong at all.
If this was one of a few that has the same or similar issues it would
make some sense and I could go to the people I work with asking them to
look into this issue. But it is the only company that has this issue.
Has anybody seen a similar type of a situation before? Understood that
you cannot fix this but would appreciate advise as to where to look so
hopefully this can be solved.
Thank you.
Bill Dworak
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|