TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 15 Jun 2009 13:45:33 EDT
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Joe Fjelstad <[log in to unmask]>
X-cc:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (72 lines)
Hi Steve
 
Seeing the "rest of the picture" helps. The first one was cut off short. (I 
 suppose that's one way to make a problem go away... ;-) 
 
Thanks
Joe 
 
 
In a message dated 6/15/2009 10:12:13 A.M. Pacific Daylight Time,  
[log in to unmask] writes:

Hi Joe,
 
I think that the  last image that Genny sent me was darker than the first 
two so that  you could see that the solder ball was soldered fine at the 
device to ball  interface and at the ball to pad interface. I don't think there 
was anything  wrong with the solder joint...
 
I believe that the  cratering she was talking about was shown in her first 
two photos in the  laminate just beneath the PCB pads
 
_http://stevezeva.homestead.com/files/crack_bright_100x.jpg_ 
(http://stevezeva.homestead.com/files/crack_bright_100x.jpg) 
 
_http://stevezeva.homestead.com/files/crack_bright_200x.jpg_ 
(http://stevezeva.homestead.com/files/crack_bright_200x.jpg) 
 
Genny, correct me if  I'm wrong?
 
Steve

 
____________________________________
 From: [log in to unmask] [mailto:[log in to unmask]]  
Sent: Monday, June 15, 2009 11:37 AM
To: Steve  Gregory
Subject: image adjusted



Hi Steve
 
I adjusted the image to see better. Other than the small voids I am  
curious what is being seen. There seems to be no cratering 
 
Cheers, 
Joe

 
____________________________________
An Excellent Credit Score is 750. _See  Yours in Just 2 Easy  Steps!_ 
(http://pr.atwola.com/promoclk/100126575x1221322979x1201367215/aol?redir=http://ww
w.freecreditreport.com/pm/default.aspx?sc=668072&hmpgID=62&bcd=JuneExcfooter
NO62) 


**************An Excellent Credit Score is 750. See Yours in Just 2 Easy 
Steps! 
(http://pr.atwola.com/promoclk/100126575x1221322979x1201367215/aol?redir=http://www.freecreditreport.com/pm/default.aspx?sc=668072&hmpgID=62&bcd=Jun
eExcfooterNO62)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2