TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Kelly <[log in to unmask]>
Date:
Wed, 10 Jun 2009 16:26:48 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Aleks Lozinsky <[log in to unmask]>
Subject:
From:
Aleks Lozinsky <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<00d901c9ea06$1741ee70$45c5cb50$@com>
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
MIME-Version:
1.0
Parts/Attachments:
text/plain (116 lines)
Hi Steve,
I think photoresist needed for two main reasons - purpose of electrolytic 
gold plating ( its selectivity) and cost of the gold.
Aleks Lozinsky
Technic Canada
----- Original Message ----- 
From: "Steve Kelly" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, June 10, 2009 4:00 PM
Subject: Re: [TN] Immersion Gold versus Electrolytic Gold


> Hi Rudy,
> We electroplate gold everyday with no photoresist- why would you need a
> photoresist in the electroplate area? Regards Steve Kelly
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak
> Sent: June-10-09 3:19 PM
> To: [log in to unmask]
> Subject: Re: [TN] Immersion Gold versus Electrolytic Gold
>
> Harris:
>
> Perhaps the single biggest difference between electrolytic and immersion
> gold, besides the self-limiting aspect of immersion gold, thus limiting
> thickness, is that immersion gold covers the entire trace, including
> sides. Electrolytic gold must be applied with a photoresist on the board,
> and thus the sides of the traces are exposed Copper.
>
> Electrolytic gold is applied on top of electrolytic Nickel MOST of the 
> time,
> there are some people doing direct gold on top of Copper, but it is quite
> thick. Plating Copper under the Nickel is unnecessary.
>
> Rudy Sedlak
> RD Chemical Company
>
> --- On Wed, 6/10/09, Harris Dy <[log in to unmask]> wrote:
>
> From: Harris Dy <[log in to unmask]>
> Subject: [TN] Immersion Gold versus Electrolytic Gold
> To: [log in to unmask]
> Date: Wednesday, June 10, 2009, 10:31 AM
>
> Hi guys,
>
> Can you please help to differentiate the two surface finishes? Also, is
> Electrolytic Gold done in Cu-Ni-Au plating line or there is another way?
>
> Thanks in advance,
> Harris
>
>
>
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2