notwithstanding the Plumbing Inspector who comes to check-up on your plumbing job you got a permit for and wants to see the solder you used. Not sure if all but many states now you have to use unleaded solder when sweating copper pipes. Tough stuff -
Randy Bock Sr.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Friday, June 05, 2009 12:50 PM
To: [log in to unmask]
Subject: Re: [TN] Flux cored wire solder shelf life
Mountain Dew will only oxide the outside. Don't ask me how I know that.
In addition to the costs outlined by Dewey, you can add in the costs and
headaches of trying to explain to your customer why you used 10 year old
solder on their product when they catch it in the audit. Sure they work,
but is it worth the hassle, no pun intended. Ok, maybe pun intended.
Doug Pauls
Rockwell Collins
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
06/05/2009 11:28 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Flux cored wire solder shelf life
If the solder was good initially and stored anywhere, except near Doug's
Mountain Dew stash, it will be good for years. The problem is the cost
of having an acceptable process for extending shelf life. In the long
run it is probably more cost effective to discard all materials that
have passed/exceeded their expiration/shelf life dates, then to
acknowledge the non-conformance, segregate, inspect, disposition the
non-conformance ( establish accept/reject criteria, re-test, re-certify,
re-label) and eventually either discard or return the materials to
stock.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, June 05, 2009 8:38 AM
To: [log in to unmask]
Subject: [TN] Flux cored wire solder shelf life
Well, we made it to Friday!
I'm going ask ya'll a couple of question that I think I know the answer
to, but I want to hear what you think.
Right now I'm in the midst of gathering up all my solder dross, expired
solder paste, and wire solder for a shipment to my recyclers. I noticed
we had a bunch of wire solder in the locker of our training room that
was really old, like it was manufactured back in February of 1997. The
alloy is 63/37, the flux core is a pretty active water soluble organic
acid.
The manufacturer says that shelf life for flux cored wire solder is
3-years. But when I took some of the solder and soldered with it, it
soldered absolutely fine. Wet and flowed out with no problems
whatsoever.
So my question is, have any of actually had any problems soldering with
flux cored wire solder because it was too old? Do you think that
manufacturers shelf life is realistic?
Steve
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|