Hi Doug,
I like your way of thinking. At my previous place of employment we did
Parylene coating and we did the .10" cross hatch tape test. We would run a
coupon of the same board material through the process and do the testing on
it. The test was sort of subjective since a pass was based on a percentage
of removed coating. A partial square, a whole square, a little bit, etc.
were always questions. It was never changed as far as I know and they always
passed the test. I still think Doug has the best answer though.
KennyB
-----Original Message-----
From: Douglas Pauls [mailto:[log in to unmask]]
Sent: Monday, May 11, 2009 4:34 AM
To: [log in to unmask]
Subject: Re: [TN] Parylene Adhesion Tape Test
Mary Lou,
I have issues with most of the tape tests, ASTM or otherwise, as the
results are far too often subjective and do not represent real world
factors. We used to use a version of the ASTM tape test here, where a
process control coupon was coated, cured, and an "X" scribed into the
coating. Tape was applied over the top and pulled off. Whether or not
you passed that test was dependent on whether Bob the Gorilla or Millie
the Mouse performed the test, was the razor blade sharp, did you snap pull
the tape, was the tape new or old, was the correct tape used....? We
stopped using that test because it created too many false positives,
showing problems where none existed.
Secondly, until Boeing or Airbus start to install small elves that run
around inside our avionics carving up the coating with razor blades, the
tape test does not represent a valid failure mechanism for the coating.
For us, as long as the conformal coating adheres through our climactic
burn in testing, then it is acceptable. Since coating adhesion generally
increases with time, if it passes temperature-humidity cycling in the
factor right after cure, it will last in the field.
Now, if we do see loss of conformal coat adhesion after cyclical testing,
then we have to track down why and determine root cause. What was the
pre-cursor to your Parylene failures?
Doug Pauls
Rockwell Collins
Mary Lou Sachenik <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/09/2009 06:47 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Mary Lou Sachenik <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Parylene Adhesion Tape Test
We recently had some issues with lack of adhesion of Parylene coating
What types of notes are being used on drawings to define parylene
conformal coating adhesion test on pwa's?
Is the ASTM3359-08 (for assessing the adhesion of coating films to
metallic substrates) the best spec to call out for this testing .
I presently don't have pwb coupons to perform destructive cross hatch
test.
What type of tape is being used testing parylene adhesion on the PWA's?
Some specs call out 3M-250 tape, the ASTM D 3359 calls out the Permacel
99.
Actually I prefer the Wescorp 79210 clear Anti-static Tape, does this seem
acceptable?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|