Well I have to say: As it's from you, that's the best thing said to me all
week, thanks!
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Whittaker, Dewey (EHCOE)
Sent: Friday, May 29, 2009 3:50 PM
To: [log in to unmask]
Subject: Re: [TN] Conformal coating process
Mike and Graham,
Kudos for no implants of humor in unsupported areas, but your sound
advice presented with a witty repertoire cuts into my area, especially
on Friday.
Graham, an admitted Teaker, I can see, but et tu Mike.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Fenner
Sent: Friday, May 29, 2009 12:54 AM
To: [log in to unmask]
Subject: Re: [TN] Conformal coating process
Yes. In the sense that the word is commonly used there are all sorts of
silicones, just as there are all sorts of other chemical families/types.
Just because one member of a particular chemical type has some
undesirable
(in this case mechanical) properties, doesn't mean they all have it. If
that
were the case you would be in trouble with everything in your building.
This started as Inge said from silicone based lubricants, these can be
very
mobile and end up in all sorts of places, sometimes by non-intuitive
routes,
and they can be concern.
I suppose you could put up a notice or two saying no Silicones past this
line to keep them happy, of course you would not be able to stick them
up
with Scotch tape. Which rather makes the point.
Regards
Mike
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Thursday, May 28, 2009 9:37 PM
To: [log in to unmask]
Subject: Re: [TN] Conformal coating process
What about all car/machine/outdoors electronics potted with silicon for
decades then? It works.
People can't distinguish between cured silicon and silicon oil. It was
the
later that started the 'silicon hysteria' about 1960.
Inge
----- Original Message -----
From: "Kane, Joseph E (US SSA)" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, May 28, 2009 10:25 PM
Subject: Re: [TN] Conformal coating process
If you haven't seen any pesky solderability problems in 15
years, then the risk is probably overstated. And if your
solder connections meet visual requirements, then your customer
has no cause for concern.
-Joe
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Johnson
Sent: Thursday, May 28, 2009 3:38 PM
To: [log in to unmask]
Subject: [TN] Conformal coating process
We are a contract builder that manufactures printed circuit board
assemblies and apply a silicone conformal coating to those assemblies.
Our coating process is not isolated from the assembly and test area. We
use a Sn63Pb37 solder process in both our smt and wave solder areas.
This has been our process for at least the last 15 years. We are being
told, by a potential customer, that we are risking silicone
contamination of our solder joints as a result of our coating process
being in close proximity to assembly and test.
What are the risks to solder joint quality, if any? Thanks.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content, and any files transmitted with it, are
intended solely for the addressee(s) and may be legally privileged
and/or confidential. If you are not the intended recipient, please
contact the sender by return and delete the material from any computer.
Any review, retransmission, dissemination, or other use of, or taking of
any action in reliance upon this information by persons or entities
other than the intended recipient is prohibited.
Messages sent via this medium may be subjected to delays, non-delivery,
and unauthorized alteration. This email has been prepared using
information believed by the author to be reliable and accurate, but
Indium Corporation makes no warranty as to accuracy or completeness.
Indium Corporation does not accept responsibility for changes made to
this email after is was sent. Any opinions or recommendations expressed
herein are solely those of the author. They may be subject to change
without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
***This email, its content, and any files transmitted with it, are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient, please contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination, or other use of, or taking of any action in reliance upon this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subjected to delays, non-delivery, and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. Indium Corporation does not accept responsibility for changes made to this email after is was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|