Rudy,
THAT was exactly what I wanted to hear. Mono-layers. I was afraid of that,
and I've told our chemists that I suspected such a scenario. We are
struggling with a laser issue, that is the only I can tell you.
Inge
----- Original Message -----
From: "R Sedlak" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, May 29, 2009 6:01 PM
Subject: Re: [TN] WAX
Inge:
Technically speaking there is a large difference between a wax and a polish.
A polish does grind down the surface, and may or may not leave a coating
behind.
A wax is primarily a coating, and often does little if any "grinding down"
of the surface.
The thickness of any coating left by either wax or polish is going to be a
function of not only composition of the wax/polish, but also how aggressive
the mechanical polishing is.
Some polishes leave only a mono-molecular film of anti-tarnish.
Rudy Sedlak
RD Chemical Company
--- On Fri, 5/29/09, Victor Hernandez <[log in to unmask]> wrote:
From: Victor Hernandez <[log in to unmask]>
Subject: Re: [TN] WAX
To: [log in to unmask]
Date: Friday, May 29, 2009, 8:24 AM
A picture is worth a thousand words.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Friday, May 29, 2009 9:34 AM
To: [log in to unmask]
Subject: [TN] WAX
Hi all and even Bev,
Assume that you polish a metal, in my case five 9s Ag. Polishes have at
least two purposes. Grind the metal to get a certain level of brightness
(we
polish to Ra 30 nanometers). And leave a thin coating that protects the
metal. Now, in our case, what is left is so thin, that you can't observe
the
'coating'. Presumably because it's an organic compound of some sort,
and
also because it's transparent for our eye's wavelength. Now comes the
question: has anyone out there ever investigated such a 'wax' and
determined the thickness, and if so, what kind of equipment was used?
That's why I more or less directed the q to Bev...
Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|