Depend on what rtv. Some rtv never inert.
--------------------------
Sent using BlackBerry
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Sun May 31 08:51:17 2009
Subject: Re: [TN] Immersion Silver
Hi,
Is there any risk after assembly, if the immersion silver PCB will be RTV
sealed in inert environment?
Which Pad to Pad Clearance required for reducing risk of electrochemical
migration ?
Anat
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Maurice Dore
Sent: Wednesday, May 27, 2009 9:36 AM
To: [log in to unmask]
Subject: Re: [TN] Immersion Silver
Steve
Good place to start is IPC4553 - Silver tarnishes in the presence of
sulfur (Ag2S forms on the surface);
a. Storage & Handling
Handling- Gloves worn by Operators at all stages of production
1. Immersion silver boards should be packaged as soon as possible, to
prevent exposure to chlorides and sulfides in the air.
2. Use sulfur free, pH neutral paper to wrap stacks of parts and then
plastic wrap. Storage should be in sealed bags or sealed containers to
eliminate direct contact with air.
3. Wrapped packages should be stored below 30°C (86°F) and 75% R.H.
4. Do not use desiccant in the packages. Desiccant can contain sulfur
compounds.
5. Adhesive tape, adhesive labels, stamps, markers and rubber bands are
forbidden on silver boards and the sulfur free paper. They all contain
sulfur bearing compounds that will tarnish the silver coating.
6. If the original package is opened and not all of the boards consumed at
the EMS/OEM, they should be re-wrapped as soon as possible and returned to
a storage condition, preferably not-to-exceed 30°C (86°F) and
75% R.H.
b. Shelf Life
- Controlled Shelf Life in unopened Vendor packaging - 6 months and 4
weeks resealed Vendor packaging
- Floor Life - Double Sided Reflow - 48 hrs max
- Floor Life - to complete all solder assembly (i.e. wave solder) - 7 Days
maximum Floor Life
c. Corrosion Prevention
- Pads are non-soldermask defined, reduces risk of any creep corrosion
? Pad to Pad Clearance reduces risk of electrochemical migration
? PCB Supplier to observe ImmAg Thickness ( 0.2 - 0.4µm )
The key is to reduce exposure time to sulfide and chlorides (remember to
check both site levels) - I noticed solderability issues after 14 days
exposure time that affects our wave soldering process. logistics of moving
between manufacturing sites should be ok if controlled as recommended.
Rgds
Moss
Steve Kelly <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
26/05/2009 22:00
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Steve Kelly <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Immersion Silver
Good Afternoon,
Any concerns about using immersion silver as a finish. PWB has to take two
reflow cycles, 1 re-work cycle and one hand solder after the two reflows.
Parts have to be transported from one part of the country to another after
the two reflows. Thanks. Steve Kelly
Steve Kelly (PLEASE NOTE NEW E-MAIL ADDRESS)
(416) 750-8433 (work)
(416) 750-0016 (fax)
(416) 577-8433 (cell)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Connaught Electronics Limited
Company registration N°92489
This e-mail message is intended only for the use of the intended
recipient(s).
The information contained therein may be confidential or privileged, and its
disclosure or reproduction is strictly prohibited.
If you are not the intended recipient, please return it immediately to its
sender at the above address and destroy it.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|