Nice one Joe
Victor here is a link describing the effect of solder mask on trace
impedance :
http://www.sigcon.com/Pubs/edn/PassivationandSolderMask.htm
As Joe alludes it is indeed a dielectric with a typical dielectric constant
value of 3.3. You will find in RF designs that often the boards are
specified without solder mask for this very reason.
Have a great weekend,
John
John Burke
(408) 515 4992
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: Friday, May 08, 2009 1:11 PM
To: [log in to unmask]
Subject: Re: [TN] Solder Mask
Victor
How/why do you conclude that solder mask is not a dielectric?
Cheers,
Joe
In a message dated 5/8/2009 12:37:48 P.M. Pacific Daylight Time,
[log in to unmask] writes:
Fellow TechNetters:
Besides being a moisture barrier and solder dam what else is the
function of solder mask. It is not a dielectric.
Victor,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
**************A Good Credit Score is 700 or Above. See yours in just 2 easy
steps!
(http://pr.atwola.com/promoclk/100126575x1221322931x1201367171/aol?redir=htt
p://www.freecreditreport.com/pm/default.aspx?sc=668072&hmpgID=115&bcd
=May5509AvgfooterNO115)
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|