TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 27 May 2009 08:30:43 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
From:
"Wenger, George M." <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (180 lines)
In order to give you an meaningful answer I think we need
Wayne,



In order to give you an meaningful answer I think we need more

information from your side.



1. Where the capacitors wave soldered or reflow soldered?

2. What type of flux was used?

3. What solvent was used?

4. What type of cleaning process was used?



Regards,

George

George M. Wenger

Andrew Solutions

Senior Principal FMA/Reliability Engineer

40 Technology Drive, Warren, NJ 07059

(908) 546-4531 (Office) (732) 309-8964 (cell)

[log in to unmask]



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Glidden

Sent: Wednesday, May 27, 2009 8:24 AM

To: [log in to unmask]

Subject: Re: [TN] humidity test failure



Looks like whatever it is it may have started from residues leaching

from

UNDER the component.  The voltage bias and environment would have only

accelerated this.   The solder joints exposed to the cleaning process

look

fine.  You should review your cleaning procedures and perform testing

(IC/SIR) to determine if you are adequately cleaning, rinsing, and

drying to

remove contaminants from under low-standoff components.  My suspicion is

that if that is in fact the case, and you decided to try to conformal

coat,

the problem would have only manifested itself sooner with conformal coat

adhesion problems.  





-----Original Message-----

From: Steve Gregory [mailto:[log in to unmask]] 

Sent: Wednesday, May 27, 2009 8:00 AM

To: [log in to unmask]

Subject: Re: [TN] humidity test failure



Good Morning!



Half the week down already. That's another nice thing about 3-day

weekends;

you also get a 4-day work week either prior to, or after the weekend.



I have Wayne's picture posted now. It's at:

 

http://stevezeva.homestead.com/files/C23_Humidity_failure.JPG



Definitely some kinda' junk there!



Steve



-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Thayer, Wayne

Sent: Tuesday, May 26, 2009 9:01 PM

To: [log in to unmask]

Subject: [TN] humidity test failure



Hi Technet Gurus!



I have attached a picture of a part responsible for excess current draw

during an extended humidity/temperature cycling test. (I copied Steve so

he

can hopefully post!)



The board was carefully solvent cleaned, but no SIR test validating the

process strips all ionic contamination.  The board is in an enclosure

where

plenty of ionic contaminants are available.



Humidity was supposed to not exceed 90% and was to be non-condensing

during

cycling.  There were a handful of components which displayed similar

deposits on the same circuit board.  These were the only parts biased

during

the humidity test.  I believe the evidence suggests at least some

condensation occurred.  To me the deposits look like salts.

But what do "the experts" think?



Is there any rule of thumb as to humidity levels where we are nuts to

try to

survive without conformal coating?  Part of the adjacent circuitry

contains

RF devices and those guys get panic-stricken when told we probably need

to

conformal coat!



Wayne Thayer



This e-mail and any files transmitted with it may be proprietary and are

intended solely for the use of the individual or entity to whom they are

addressed. If you have received this e-mail in error please notify the

sender.

Please note that any views or opinions presented in this e-mail are

solely

those of the author and do not necessarily represent those of ITT

Corporation. The recipient should check this e-mail and any attachments

for

the presence of viruses. ITT accepts no liability for any damage caused

by

any virus transmitted by this e-mail.



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

unsubscribe, send a message to [log in to unmask] with following text in

the

BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet

NOMAIL or (MAIL) To receive ONE mailing per day of all the

posts: send e-mail to [log in to unmask]: SET Technet Digest Search the

archives of previous posts at: http://listserv.ipc.org/archives Please

visit

IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for

additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

unsubscribe, send a message to [log in to unmask] with following text in

the

BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or

(re-start) delivery of Technet send e-mail to [log in to unmask]: SET

Technet

NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send

e-mail to [log in to unmask]: SET Technet Digest Search the archives of

previous posts at: http://listserv.ipc.org/archives Please visit IPC web

site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at:

http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

-----------------------------------------------------



------------------------------------------------------------------------------------------------

This message is for the designated recipient only and may

contain privileged, proprietary, or otherwise private information.  

If you have received it in error, please notify the sender

immediately and delete the original.  Any unauthorized use of

this email is prohibited.

------------------------------------------------------------------------------------------------

[mf2]



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2