TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 13 May 2009 12:08:18 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Douglas Erb <[log in to unmask]>
Subject:
From:
Douglas Erb <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (133 lines)
Genny and Lee,
Pre solder "Bake-out" has become SOP since the introduction of solder
reflow techniques.  Note: I am not aware of any Polyamides that can
handle some of the higher reflow temps being specified by many OEMs, but
Hirose has many products that are successfully applied at 240-C to 245-C
all over the world.  The generic 260-C will cause event the best
Polyamides to warp, or worse.  The key here is the temp measured at the
board/component level, not ambient atmosphere.

I was going with 1946, myself, but pulled that out of thin air.  :-)

Doug Erb
Senior FAE
Hirose USA

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman
Sent: Wednesday, May 13, 2009 11:58 AM
To: [log in to unmask]
Subject: Re: [TN] Nylon connectors - moisture sensitivity

Genny,

Echoing Doug's statement (my boss delayed me again), I recently had a
colleague from a different site tell me that they bake out their
hardware at 85C-125C for over 1 hour to remove all moisture from nylon
connectors and fittings.

Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Erb
Sent: Wednesday, May 13, 2009 2:50 PM
To: [log in to unmask]
Subject: Re: [TN] Nylon connectors - moisture sensitivity

Genny,
It depends upon the type of Nylon being used.  In general Nylon is
hydroscopic and not a good choice for moisture rich environments.  Some
of the new compounds that have improved heat resistance are also more
moisture resistant, but still can cause problems.
If you are concerned only about post solder wash, this should not be an
issue, but you should make certain that the assembly is thoroughly
dried.  I hope that this helps.

Doug Erb
Senior FAE
Hirose USA
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Wednesday, May 13, 2009 11:43 AM
To: [log in to unmask]
Subject: [TN] Nylon connectors - moisture sensitivity

We have been told that a surface mount nylon connector we use is
moisture sensitive, and should be treated as equivalent to level 5a.
This is the highest level we have ever seen on any component we have
used of any type.  I didn't think that a connector could be moisture
sensitive.  Not heat tolerant, yes - we have melted a few - but moisture
sensitive?  
What kind of damage can happen to a nylon connector from too much
moisture absorption?
Thanks in advance for your responses.

Genny 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2