TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 12 May 2009 10:33:34 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Lamar Young <[log in to unmask]>
Subject:
From:
Lamar Young <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (123 lines)
Rich,

That is correct.  We call it a 'Pick Test'.  It allows one to test a much 
smaller area than with the tape test method.  It is still somewhat 
subjective, eventhough a number is assigned.  But, once the tester 
experiences the different ranges of adhesion, there will be little doubt 
as to what a '0' is (no adhesion), or a '5' (can't remove).  There may be 
some discussion as to if a value is a 2 or 3. 
The benefit is that it is a simple test that anyone can perform without 
any special equipment.

There are special tools that are nanoindenters/stylus systems that apply a 
downward pressure as the stylus moves along the surface.  It is possible 
to get quantifiable results as to the forces necessary to cause a 
separation at the coating/substrate interface.  But, it is only a number, 
it doesn't tell if it is good or bad.  It has to be compared with a sample 
that is good and bad to understand what the pass/fail results are.  The 
downside is that these systems are specialized and can be expensive, close 
to 6 figures or more.

Lamar





Richard Kraszewski <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
05/12/2009 10:06 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Richard Kraszewski <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Parylene Adhesion Tape Test






At last Falls IPC Cleaning Symposium in Rosemont, IL  Lamar Young / SCS
presented a paper where he wasn't using tape, but rather lifting the
squares with a needle and assessing the adhesion using a Likert scale.
He claimed the results were more consistent than tape.  I think that the
testing for that presentation was actually done on parylene.

You should be able to find the proceedings somewhere in IPC. 


Rich Kraszewski / PLEXUS


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mary Lou Sachenik
Sent: Saturday, May 09, 2009 6:48 AM
To: [log in to unmask]
Subject: [TN] Parylene Adhesion Tape Test

We recently had some issues with lack of adhesion of Parylene coating

What types of notes are being used on drawings to define parylene
conformal coating adhesion test on pwa's?
Is the ASTM3359-08 (for assessing the adhesion of coating films to
metallic substrates) the best spec to call out for this testing .
I presently don't have pwb coupons to perform destructive cross hatch
test.

What type of tape is being used testing parylene adhesion on the PWA's? 
Some specs call out 3M-250 tape, the ASTM D 3359 calls out the Permacel
99.
Actually I prefer the Wescorp 79210 clear Anti-static Tape, does this
seem acceptable?

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


Confidentiality Note: This e-mail message and any attachments may contain 
confidential or privileged information. If you are not the intended 
recipient, please notify me immediately by replying to this message. 
Please destroy all copies of this message and any attachments. Thank you.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2