Graham,
With some luck, Dewey is slacking off.
Werner
-----Original Message-----
From: [log in to unmask]
To: [log in to unmask]; [log in to unmask]
Sent: Wed, 20 May 2009 7:06 am
Subject: RE: [TN] Underfill Pass/fail criteria
Well, if I knew I was not clear on it does that make me just half
dumb, or full dumb??? Dewey, cut me some slack!!!
Thanks Werner.
regards,
- Graham
From: [log in to unmask]
[mailto:[log in to unmask]]
Sent: Tuesday, May 19, 2009 4:29 PM
To: Collins, Graham (FN) @ ESI; [log in to unmask]
Subject: Re: [TN] Underfill Pass/fail criteria
Hi Graham,
You are reading it incorrectly.
If you
compare the results in Fig. 2 with those in Figs. 3 and 4, it is clear that
snap-curing underfill give better fatigue life improvements [do not ask me why,
I don't know].
Werner
-----Original Message-----
From: [log in to unmask]
To: [log in to unmask]; [log in to unmask]
Sent: Tue, 19 May 2009 3:17 pm
Subject: RE: [TN] Underfill Pass/fail criteria
Werner, my apologies - if I have offended it was not intended –
where meaning has not been understood the fault is mine. Well, that and
plus that just as I think I’m understanding the intent of what you’ve written,
someone rushes into my cube and distracts me with an inane
fact.
The one thing I’m not clear on – you seem to be saying tha t slow
curing resins give a better fatigue life, but that this doesn’t translate into
real-world reliability improvement? Or am I reading it incorrectly?
regards,
- Graham Collins
From: [log in to unmask]
[mailto:[log in to unmask]]
Sent: Tuesday, May 19, 2009 4:01 PM
To: [log in to unmask];
Collins, Graham (FN) @ ESI
Subject: Re: [TN] Underfill Pass/fail criteria
Hi Graham,
The English language is wonderfully adapt to explain things—that is why it has
displaced French as the language of diplo macy and German as the language of
technology—it is now a great lingua franca.
I try [nobody is perfect, as my wife reminds me all the time], but sometimes I
do not succeed in conveying the meaning properly.
What do I need to clarify, if not to say dumb down?
Werner
-----Original Message-----
From: Graham Collins <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, 19 May 2009 2:31 pm
Subject: Re: [TN] Underfill Pass/fail criteria
For the rest of us, it's possible to get a copy of Werner's article at:
http://www.globa
lsmt.net/index.php?option=com_content&task=view&id=33&Itemid=65
Now if only I could get him to explain it to me in small words... :-)
regards,
- Graham Collins
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier /*
Sent: Tuesday, May 19, 2009 3:18 PM
To: [log in to unmask]
Subject: Re: [TN] Underfill Pass/fail criteria
Hi Bev,
Clearly, the most important SJs that need to be covered are the outermost rows
and the rows directly underneath the die outline—this later is most important
for face-up BGAs and CSPs.
=0
A
I do not know if one can
write generally applicable pass/fail criteria [because,
what else, 'It depends'].
I ave attached a column of mine on underfills [sorry for the rest of you for
whom IPC strips the attachment], Engelmaier, W., “Reliability Improvement with
Underfill,” Global SMT & Packaging, Vol. 6, No. 3, March202006, pp. 66-67.
Werner
-----Original Message-----
From: Bev Christian <[log in to unmask]>
To: [log in to unmask]
Sent: Tue, 19 May 2009 1:51 pm
Subject: [TN] Underfill Pass/fail criteria
0A
TechNetters,
I am aware of J-STd-030 "Guideline for Selection & Application of
Underfill" and the existence of IPC standards committee 5-24F "Underfill
Adhesives for Flip Chip Applications". There is nothing in IPC-A-610D
about underfills. I have taken Brian Toleno's very good course on
underfills, but on going back and looking at the CD, I don't see
anything on pass/fail criteria. Do any of you know of an international
standard (American, IEC, Japanese) with pass/fail criteria for cured
unde
rfills?
I am particularly interested in what said standard (or
anything you want
to tell me) says about coverage and voiding.
Bev
RIM
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged
material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error, please
immediately reply to the sender and delete this information from your system.
Use, dissemination, distribution, or reproduction of this transmission by
unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visi
t IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per20day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-710
0 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|