We recently had some issues with lack of adhesion of Parylene coating
What types of notes are being used on drawings to define parylene
conformal coating adhesion test on pwa's?
Is the ASTM3359-08 (for assessing the adhesion of coating films to
metallic substrates) the best spec to call out for this testing .
I presently don't have pwb coupons to perform destructive cross hatch
test.
What type of tape is being used testing parylene adhesion on the PWA's?
Some specs call out 3M-250 tape, the ASTM D 3359 calls out the Permacel
99.
Actually I prefer the Wescorp 79210 clear Anti-static Tape, does this seem
acceptable?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------