TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 29 May 2009 15:39:02 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, John Burke <[log in to unmask]>
Subject:
From:
John Burke <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (157 lines)
I know Joyce I am looking at it - those "tight" designs my engineering team
keep throwing at me may lead to the point where I have to use it.


John Burke
(408) 515 4992


-----Original Message-----
From: Joyce Koo [mailto:[log in to unmask]] 
Sent: Friday, May 29, 2009 3:28 PM
To: [log in to unmask]; [log in to unmask]
Subject: Re: [TN] WAX

John, the coating is not patented.  It is trade secret.  You can use regular
wire ball bonder to bond 30 micron or less with multi tire die stack in high
speed.  You can form a ball without residue form the ball bond and no
coating flake off or evaporation residue on gold pad.  Not a simple "wax"
;-) to me. 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Fri May 29 16:52:30 2009
Subject: Re: [TN] WAX

Interesting......... they got a patent on insulating solid core conductor
wire????????? Someone should go patent the butt to make sure they never sit
down again at the patents office.

John Burke
(408) 515 4992

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Friday, May 29, 2009 8:56 AM
To: [log in to unmask]
Subject: Re: [TN] WAX

Inge,
Nope I haven't.  But, Joyce, who is at ECTC right now, may be able to
shed some light on this from her time at Microbonds, where their main
patent deals with putting a coating on gold bond wires that allows them
to touch without shorting out.

On a shiny surface like that you MIGHT be able to determine
presence/absence by FTIR, but maybe not because of the thin nature of
the film.  Certainly we have not been able to confirm the presence of
material in water spots on gold surfaces.

Two techniques that come to mine to try and Auger and/or XPS, but I am
not even a novice in either technique.  Both are very expensive.
Regards,
Bev
RIM  

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Friday, May 29, 2009 10:34 AM
To: [log in to unmask]
Subject: [TN] WAX

Hi all and even Bev,

Assume that you polish a metal, in my case five 9s Ag. Polishes have at 
least two purposes. Grind the metal to get a certain level of brightness
(we 
polish to Ra 30 nanometers). And leave a thin coating that protects the 
metal. Now, in our case, what is left is so thin, that you can't observe
the 
'coating'.  Presumably because it's an organic compound of some sort,
and 
also because it's transparent for our eye's wavelength. Now comes the 
question:  has anyone out there ever investigated such a 'wax' and 
determined the thickness, and if so, what kind of equipment was used? 
That's why I more or less directed the q to Bev...

Inge 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2