Hi Charming,
What is the surface finish on the PWB?
Paul Reid
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Charming Chan
Sent: Friday, May 29, 2009 4:46 AM
To: [log in to unmask]
Subject: [TN] Looking for opinions on separation/delamination between
copper land and dielectric material.
Hello All,
Our guys ran a thermal shock test to verify solder joint reliability of
a TSSOP component. The micro-section shows that there is a minor crack
at the toe side of the solder joint and a separation(delamination)
between the copper land and the dielectric material.
My question is,
Where did the separation/delamination occur? PCB fab house, PCB assembly
house, or thermal shock test?
If the separation/delamination occurred at pcb fab house, then, what's
the possible root cause gonna be?
If the separation/delamination occurred at thermal shock test or pcb
assembly house, then, is it caused by CTE mismatch between pcb base
material, solder alloy, and gull-wing footprint? How to improve on that?
Brain storm, and any input is appreciated.
I will get the micro-section picture posted once I get it. Thank you
all.
Best Regards
Charming Chan
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|