TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 20 May 2009 21:56:11 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
From:
Parts/Attachments:
text/plain (21 lines)
Since early 60s it was decided that 5,000 ppmv moisture was maximum allowed 
for hermetic packages. Corresponds to a number of monolayers water on the 
chip or substrates. Converted to about 1um of leakage hole and molecular 
Helium flow it means 5x10exp-8 atm cc per sec. If you seal with maximum 10 
ppmv O2 this will give 10 years without getting dewpoint over the dangerous 
level. However, with 1 volt chips and line space as little as 0.1 um, and 
life expectancy as much as 20 years or more the old limits are questionable 
by many. Some recommend a level of exp-11. Then we leave molecular flow and 
goes to diffusion . Have anyone of you implemented that ?
Inge 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2