Thanks Bob. I have just talked to Brian Toleno and David Hillman here at the conference here in Toronto. We will marry that to what the three of us have committed to share. I think we are finally on our way to a standard!
Bev
RIM
----- Original Message -----
From: Bob Willis <[log in to unmask]>
To: 'TechNet E-Mail Forum' <[log in to unmask]>; Bev Christian
Sent: Wed May 20 06:44:11 2009
Subject: RE: [TN] Underfill Pass/fail criteria
Working in South Africa at the moment but I did produce a standard or some
guidelines some years back for Speedline Workshop. I will circulate a link
when I get back to my office providing I can still find it.
I always wanted to do this and produce a set of images to go with my
underfill workshop.
Send the link to all when I get away from the sharks!!
Bob Willis
2 Fourth Ave, Chelmsford, Essex, CM1 4HA England
Tel: (44) 1245 351502
Fax: (44) 1245 496123
Mobile: 07860 775858
www.ASKbobwillis.com
PCB Design for Manufacture & Assembly Workshop 15th October
www.ASKbobwillis.com
PCB Inspection & Quality Control Workshop 3rd November
www.ASKbobwillis.com/faworkshops.pdf
Book Bob's "Step by Step Failure Analysis Workshop" 4th November
www.ASKbobwillis.com/faworkshops.pdf
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: 19 May 2009 18:52
To: [log in to unmask]
Subject: [TN] Underfill Pass/fail criteria
TechNetters,
I am aware of J-STd-030 "Guideline for Selection & Application of
Underfill" and the existence of IPC standards committee 5-24F "Underfill
Adhesives for Flip Chip Applications". There is nothing in IPC-A-610D
about underfills. I have taken Brian Toleno's very good course on
underfills, but on going back and looking at the CD, I don't see
anything on pass/fail criteria. Do any of you know of an international
standard (American, IEC, Japanese) with pass/fail criteria for cured
underfills?
I am particularly interested in what said standard (or anything you want
to tell me) says about coverage and voiding.
Bev
RIM
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|