Dewey, there is a difference between normal static and marriage static.
Lots of things will dissipate normal static. Roses are the only thing
that I have found that dissipate marriage static, at least that I can
afford.
The answer to the question of having a permanent static dissipative
surface from a coating is of course "It Depends". I have done some
evaluations of Techspray Licron and like it. It does make a surface
fairly static dissipative, but does not have very good chemical
resistance. So for normal wear and tear it might be OK, but if there are
any chemicals being used in the area, like flux, flux cleaners, coatings,
thinners, etc., then probably not.
Doug Pauls
Rockwell Collins
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
04/29/2009 12:15 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] STATIC DISSIPATIVE COATINGS
Do you mean besides a Wedding Tux?
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Whiteman
Sent: Wednesday, April 29, 2009 10:08 AM
To: [log in to unmask]
Subject: [TN] STATIC DISSIPATIVE COATINGS
Has anyone ever used static dissipative coatings?
There is a coating manufacturer whose claims that their coating when
applied will make a fixture permanently static dissipative.
Any thoughts?
Thanks...
Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|