TECHNET Archives

April 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Peter Vigneau <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Peter Vigneau <[log in to unmask]>
Date:
Fri, 3 Apr 2009 13:04:46 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (77 lines)
Hi Gary,

If my assumption is correct, you have bare copper card edge fingers on your PCB assemblies. This can be fixed per IPC 7721B Modification and Repair 4.6.3 Edge Contact Repair, Plating Method. To see the procedure you can check-out the link below:

http://www.circuitrework.com/guides/4-6-3.shtml

Hope this helps.

Peter Vigneau
General Manager
[log in to unmask]
Phone: 978-478-5101
 
Circuit Technology Center
135 Ward Hill Avenue
Haverhill, MA 01835
Web:    www.circuitrework.com
Phone: 978-374-5000
Fax:   978-372-5700 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gary Camac
Sent: Friday, April 03, 2009 12:39 PM
To: [log in to unmask]
Subject: [TN] Edge connector repair

Good morning all,

 

Here's the scenario - I have assemblies that should have Ni/Au plating
on edge connector but don't; the assemblies are built; can repairs be
made?

 

Thanks in advance, 

 

Gary Camac

Senior Manufacturing Engineer

DICKEY-john Corp.

5200 Dickey John Road

Auburn, IL 62616-0010

Telephone 217-438-2288

[log in to unmask]

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2