There are too many variables at play to make blanket statements. What
die size, paste stencil thickness, board material, Pb free or SnPb, mold
compound, temperature cycles (ramp & dwell times, temp extremes), are
the signals near the die edges active or redundant, etc? I've done a
good bit of thermal cycling of leadless devices like MLF/QFN and LGA
(mostly -40/+125C) and have found that reliability is very device
dependent - sometimes in very counterintuitive ways. Some last a couple
hundred cycles and some go for thousands. I've been surprised enough
times that I've resigned myself to building coupons and performing
thermal cycling when new ones come along. Although if I got organized I
could turn the Weibull plots over to our modeling guys and save myself
some future work.
A long winded way of saying, "it depends". Sorry.
Scott Post
P.O.U. 1130-OK14-FABIII
2151 E. Lincoln Road
Kokomo, Indiana 46904-9005
765-451-2983 (Phone)
765-451-0287 (FAX)
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Thursday, April 16, 2009 6:32 AM
To: [log in to unmask]
Subject: [TN] LGAs in a military environment?
Hello Technet!
One of our designers is advocating using a LGA component in a military
product. Anyone out there doing it? I'm wondering (worried) about the
reliability since it has a very low standoff. And cleaning issues?
An example of the parts I'm referring to:
http://www.linear.com/designtools/packaging/lga/05081807_a_lga66.pdf
A Linear Technologies p/n LTM4604
regards,
Graham Collins
Halifax Production Engineering
(902) 873-2000 ext. 6215
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
************************************************************************
****************
Note: If the reader of this message is not the intended recipient, or
an employee or agent responsible for delivering this message to the
intended recipient, you are hereby notified that any dissemination,
distribution or copying of this communication is strictly prohibited. If
you have received this communication in error, please notify us
immediately by replying to the message and deleting it from your
computer. Thank you.
************************************************************************
****************
****************************************************************************************
Note: If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you.
****************************************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|