Hi Roger - there are three elements that have been shown to form whiskers:
cadmium, zinc and tin. Tin is the most famous but there are numerous cases
of both zinc and cadmium whiskers too. Check out the NASA Goddard whisker
website for examples of each.
Dave
"EIMCNews" <[log in to unmask]>
04/24/2009 10:44 AM
To
"'TechNet E-Mail Forum'" <[log in to unmask]>, <[log in to unmask]>
cc
Subject
RE: [TN] Plating on screws
Dave,
I've been around plating a lot, especially zinc and I never heard of zinc
whisker formation. Are you sure you don't mean tin whisker
formation?
If you really do mean zinc please direct me to some information about it.
It's never too late in life to learn something new.
Sincerely,
Roger Mouton
EIMC - Advanced Plating Technologies
949 481-5194
www.smartcatshield.com
[log in to unmask]
Notice of Confidentiality
The information contained in and transmitted with this email may be
confidential and is intended only for the individual or entity named
above.
If you are not the intended recipient, you are hereby notified that
inadvertent disclosure of this information to you does not constitute a
waiver of confidentiality privilege and that any review, disclosure,
copying, or use of the contents of the email by you is prohibited.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|