Hi Amol
Why only dip & look? Why not force measurement?
Graham Naisbitt
Gen3 Systems
www.gen3systems.com
On 23 Apr 2009, at 16:45, Kane, Amol (349) wrote:
> Thanks Denny. Specifically, I was looking for the names of equipment
> manufacturers in the US who manufacture Steam Ageing chambers and
> the solderability testing equipment (dip and look)
>
> Thanks,
> Amol
>
> From: [log in to unmask] [mailto:[log in to unmask]]
> Sent: Thursday, April 23, 2009 11:03 AM
> To: [log in to unmask]; Kane, Amol (349)
> Subject: Re: [TN] IPC/EIA-J-STD 002 Steam Ageing
>
> Amol,
>
> You are going to get it from Dave Hillman, chairman of IPC 002!!!
> He likes to refer to it as "steam conditioning" or "steam
> stressing". People try to equate performanc in steam stressing to
> the aging of the component in storage. Storage in Singapore is far
> different from storage in Winnepeg.
>
> Is there some part of this paragraph on equipment that is a problem?
> 3.3.1 Steam Conditioning Apparatus The steam conditioning chamber
> shall be constructed of non-corrodible materials such as
> borosilicate glass, quartz glass, stainless steel or PTFE. The
> specimen holder shall be non-reactive to prevent galvanic corrosion.
> The
> container should be insulated. The steam temperature at the
> conditioning level shall be maintained per the requirements of Table
> 3-2.
> Table 3-2 Steam Temperature Requirements
> Altitude Average Local
> Boiling Point °C
> Steam Temperature
> Limits °C
> 0-305 m 100 93 ± 3
> 305-610 m 99 92 ± 3
> 610-914 m 98 91 ± 3
> 914-1219 m 97 90 ± 3
> 1219-1524 m 96 89 ± 3
> 1524-1829 m 95 88 ± 3
> A safe means to prevent excessive pressure and a means of
> maintaining adequate water level shall be provided. Neither shall
> cause
> the vapor to cool below the specified temperature. Condensate shall
> drip freely back to the water. Care should be taken to minimize
> contact between the condensate and the specimens.
>
> Fin ally, do you have comment on either dip-and-look or wetting
> balance to measure solderability?
>
> Denny Fritz
> MacDermid, Inc
> -----Original Message-----
> From: Kane, Amol (349) <[log in to unmask]>
> To: [log in to unmask]
> Sent: Thu, 23 Apr 2009 9:37 am
> Subject: [TN] IPC/EIA-J-STD 002 Steam Ageing
>
> Dear Technetters,
>
> How are people in the industry complying with the category 3, test
> method A, B
>
> or C of this requirement for high reliability applications? the 002
> standard
>
> calls out for steam ageing and then solderability testing for
> components. What
>
> equipment is being used for steam ageing and solderability testing?
> I would
>
> appreciate any direction on this matter (on the forum or offline if
> somebody so
>
> desires)
>
>
>
> Thanks,
>
> Amol
>
>
>
>
>
>
>
>
>
>
>
> WARNING: Export Control
>
> This document may contain technical data within the definition of the
>
> International Traffic in Arms Regulations (ITAR), and subject to the
> Export
>
> Control Laws of the U.S. Government. Transfer of such data by any
> means to a
>
> foreign person, whether in the United States or abroad, without
> proper export
>
> authorization or other approval from the U.S. Department of State is
>
> prohibited.
>
>
>
> CONFIDENTIALITY NOTICE:
>
> This e-mail, and any attachments, is for the sole use of the intend
>
> ed
>
> recipient(s) and may contain information that is confidential and
>
> protected from disclosure under the law. Any unauthorized review, use,
>
> disclosure, or distribution is prohibited. If you are not the intended
>
> recipient, please contact the sender by reply e-mail, and delete/
> destroy
>
> all copies of the original message and attachments.
>
> Thank you.
>
>
>
> ---------------------------------------------------
>
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>
> To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]
> > with following text in
>
> the BODY (NOT the subject field): SIGNOFF Technet
>
> To temporarily halt or (re-start) delivery of Technet send e-mail to
>
> [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or
> (MAIL)
>
> To receive ONE mailing per day of all the posts: send e-mail to
>
> [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
>
> Search the archives of previous posts at: http://listserv.ipc.org/archives
>
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for
>
> additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]
> > or
>
> 847-615-7100 ext.2815
>
> -----------------------------------------------------
>
> ________________________________
> Green cleaning products -- do they work as well? Find out now!<http://home.aol.com/new_in_home/photogallerytall/_a/spring-cleaning-products-put-to-the-test/20090407180609990001?ncid=emlweushome00000001
> >
>
>
>
> WARNING: Export Control
> This document may contain technical data within the definition of the
> International Traffic in Arms Regulations (ITAR), and subject to the
> Export
> Control Laws of the U.S. Government. Transfer of such data by any
> means to a
> foreign person, whether in the United States or abroad, without
> proper export
> authorization or other approval from the U.S. Department of State is
> prohibited.
>
> CONFIDENTIALITY NOTICE:
> This e-mail, and any attachments, is for the sole use of the intended
> recipient(s) and may contain information that is confidential and
> protected from disclosure under the law. Any unauthorized review, use,
> disclosure, or distribution is prohibited. If you are not the intended
> recipient, please contact the sender by reply e-mail, and delete/
> destroy
> all copies of the original message and attachments.
> Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|