Hi Karen - Yes, the JSTD-002 and JSTD-003 use the same fluxes. Just a
point of clarification - both specifications have very specific flux
formulations and using "an ROL1" flux may not put you in compliance with
the specification flux requirements. Standard flux #1 and #2 are defined
in detail in the specifications so make sure the flux you are going to use
is compliant with those requirements (see Appendix E for additional
assistance).
Dave Hillman
Rockwell Collins
[log in to unmask]
Karen Tellefsen <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
03/27/2009 12:08 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Karen Tellefsen <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] Solderability fluxes
Are the ROL1 solderability fluxes specified in the current J STD 002 the
same as those in the current J STD 003?
Thanks
Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------