Amol,
You are going to get it from Dave Hillman, chairman of IPC 002!!! He likes to refer to it as "steam conditioning" or "steam stressing". People try to equate performanc in steam stressing to the aging of the component in storage. Storage in Singapore is far different from storage in Winnepeg.
Is there some part of this paragraph on equipment that is a problem?
3.3.1 Steam Conditioning Apparatus The steam conditioning chamber shall be constructed of non-corrodible materials such as
borosilicate glass, quartz glass, stainless steel or PTFE. The specimen holder shall be non-reactive to prevent galvanic corrosion. The
container should be insulated. The steam temperature at the conditioning level shall be maintained per the requirements of Table 3-2.
The steam conditioning chamber shall be constructed of non-corrodible materials such as
borosilicate glass, quartz glass, stainless steel or PTFE. The specimen holder shall be non-reactive to prevent galvanic corrosion. The
container should be insulated. The steam temperature at the conditioning level shall be maintained per the requirements of Table 3-2.
shall be non-reactive to prevent galvanic corrosion. The
container should be insulated. The steam temperature at the conditioning level shall be maintained per the requirements of Table 3-2.
shall be maintained per the requirements of Table 3-2.
Table 3-2 Steam Temperature Requirements
Altitude Average Local
Boiling Point °C
Steam Temperature
Limits °C
0-305 m 100 93 ± 3
305-61
0 m 99 92 ± 3
610-914 m 98 91 ± 3
914-1219 m 97 90 ± 3
1219-1524 m 96 89 ± 3
1524-1829 m 95 88 ± 3
A safe means to prevent excessive pressure and a means of maintaining adequate water level shall be provided. Neither shall cause
the vapor to cool below the specified temperature. Condensate shall drip freely back to the water. Care should be taken to minimize
contact between the condensate and the specimens.
shall be provided. Neither shall cause
the vapor to cool below the specified temperature. Condensate shall drip freely back to the water. Care should be taken to minimize
contact between the condensate and the specimens.
shall drip freely back to the water. Care should be taken to minimize
contact between the condensate and the specimens.
Finally, do you have comment on either dip-and-look or wetting balance to measure solderability?
Denny Fritz
MacDermid, Inc
-----Original Message-----
From: Kane, Amol (349) <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, 23 Apr 2009 9:37 am
Subject: [TN] IPC/EIA-J-STD 002 Steam Ageing
Dear Technetters,
ow are people in the industry complying with the category 3, test method A, B
r C of this requirement for high reliability applications? the 002 standard
alls out for steam ageing and then solderability testing for components. What
quipment is being used for steam ageing and solderability testing? I would
ppreciate any direction on this matter (on the forum or offline if somebody so
esires)
Thanks,
mol
WARNING: Export Control
his document may contain technical data within the definition of the
nternational Traffic in Arms Regulations (ITAR), and subject to the Export
ontrol Laws of the U.S. Government. Transfer of such data by any means to a
oreign person, whether in the United States or abroad, without proper export
uthorization or other approval from the U.S. Department of State is
rohibited.
ONFIDENTIALITY NOTICE:
his e-mail, and any attachments, is for the sole use of the intended
ecipient(s) and may contain information that is confidential and
rotected from disclosure under the law. Any unauthorized review, use,
isclosure, or distribution is prohibited. If you are not the intended
ecipient, please contact the sender by reply e-mail, and delete/destroy
ll copies of the original message and attachments.
hank you.
---------------------------------------------------
echnet Mail List provided as a service by IPC using LISTSERV 15.0
o unsubscribe, send a message to [log in to unmask] with following text in
he BODY (NOT the subject field): SIGNOFF Technet
o temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
o receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
earch the archives of previous posts at: http://listserv.ipc.org/archives
lease visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
dditional information, or contact Keach Sasamori at [log in to unmask] or
47-615-7100 ext.2815
--------
--------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|