Paul,
Joint strength is not the issue in any case. It is creep-fatigue of the SJs and that comes from the thermal expansion mismatch of the die inside the LGA and the FR-4 PCB. And remember, even so-called benign environments, like consumer products can see delta-T's of up to 80 C [-20 in winter outside to 60 C inside a car], but even Summer use [20 C to 60 C] results in delta-T's of 40 C.
Werner
-----Original Message-----
From: Paul Edwards <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, 16 Apr 2009 1:11 pm
Subject: Re: [TN] LGAs in a military environment?
Graham,
We don't and we don't even recommend it for commercial apps...
BUT... AGAIN... It all depends ...
You might want to use it in a none-critical redundant secondary system...
But even then with care...
Apart from the issues already mentioned... The critical element that the solder
joint is a surface adhesion only joint whose quality can not be determined
without damage to the joint... Yes you can x-ray it or use acoustical microscopy
to determine the voiding but this will not determine the joint strength just
that you have maximized the joint surface area...
Paul
Paul Edwards
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Collins
Sent: Thursday, April 16, 2009 3:32 AM
To: [log in to unmask]
Subject: [TN] LGAs in a military environment?
Hello Technet!
One of our designers is advocating using a LGA component in a military
product. Anyone out there doing it? I'm wondering (worried) about the
reliability since it has a very low standoff. And cleaning issues?
An example of the parts I'm referring to:
http://www.linear.com/designtools/packaging/lga/05081807_a_lga66.pdf
A Linear Technologies p/n LTM4604
regards,
Graham Collins
Halifax Production Engineering
(902) 873-2000 ext. 6215
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
=============================================================================
This email and any attachments thereto may contain private, confidential, and
privileged material for the sole use of the intended recipient. Any review,
copying,
or distribution of this email (or any attachments thereto) by others is strictly
prohibited.
If you are not the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this email and
any attachments thereto.
=============================================================================
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|