We do this all the time with capacitors mostly. Print paste, place, dispense
paste, hand-place, reflow. No need to hand solder after reflow.
I do agree with the observation about power handling. It is probably not
doubled.
Guy
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Cindy S. Bohler
Sent: Friday, April 24, 2009 6:35 PM
To: [log in to unmask]
Subject: [TN] Component stacking
These are 2515 resitors stacked. Has anyone ever tried this or seen it
done?
We would paste and reflow the bottom one, as normal. Then we would solder
the top one to the bottom one with wire and then epoxy the two of them
together. Any thoughts or suggestions?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|