TECHNET Archives

April 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Cindy S. Bohler" <[log in to unmask]>
Date:
Sun, 26 Apr 2009 13:48:25 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
John Goulet <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=utf-8
MIME-Version:
1.0
Parts/Attachments:
text/plain (34 lines)
Physically and from a design point it can be done but I would contact the component manufacturer to question the reliability and ability of the bottom resistor to maintain the rated value when the heat distribution has been blocked by the upper component. 

They may suggest a thermal epoxy to transfer the heat up so the two bodies act as one rather than a regular epoxy that would insulate the top of the part. 
----- Original Message ----- 
From: "Cindy S. Bohler" <[log in to unmask]> 
To: [log in to unmask] 
Sent: Friday, April 24, 2009 6:35:07 PM GMT -05:00 US/Canada Eastern 
Subject: [TN] Component stacking 

These are 2515 resitors stacked.  Has anyone ever tried this or seen it done?   
We would paste and reflow the bottom one, as normal.  Then we would solder 
the top one to the bottom one with wire and then epoxy the two of them 
together.  Any thoughts or suggestions? 

--------------------------------------------------- 
Technet Mail List provided as a service by IPC using LISTSERV 15.0 
To unsubscribe, send a message to [log in to unmask] with following text in 
the BODY (NOT the subject field): SIGNOFF Technet 
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) 
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest 
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 
----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2