Hi Suganthi!
What comes to mind immediately:
-What are the TSSOP pins made of? If they are one of the stiff, old style leadframe alloys like Alloy 42, then probably no issues. But if they are a newer, higher copper content alloy, then the unsoldered pin is in danger of being bent somewhere you probably won't want it.
-Solder mask is not an insulator--it is just designed to inhibit solder wetting. So there is still a chance of the NC pin making contact to whatever conductor you put in place of the pad for the NC pin.
-If you break off the NC pin as part of your process, then I see no issue unless the device has only two pins left on the side where you aren't soldering the NC pin. Obviously if there is only one weak pin left on that side, you need to be concerned as to whether too much force will be put on that remaining pin due to cleaning and other handling.
Wayne Thayer
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Selva Suganthi
Sent: Monday, April 20, 2009 2:04 AM
To: [log in to unmask]
Subject: [TN] Help me - NC pin without pad on the pcb
Dear All
My layout has a tssop pacakage which doesn't have a pad for 1 NC pin( Intentional design, there is a need to have space near to this pin.) , My Quality head has stopped the production and says this is not accepted , because of this we need to go for an another revision where there is no time in the project plan .
Actually I wanted to convince my quality team, before that I want to make clear myself abou the known issues / rules behind it. .Pls help me Techies
In this scenario what kind of a problem can we expect ?
Thanks in Advance.
Have a great day ahead.
Thanks and Regards
Suganthi,CID
"Do not go where the path may Lead, Go instead where there is no path, and leave a trail ! "
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
This e-mail and any files transmitted with it may be proprietary and are intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender.
Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Corporation. The recipient should check this e-mail and any attachments for the presence of viruses. ITT accepts no liability for any damage caused by any virus transmitted by this e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|