TECHNET Archives

April 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Richard D. Stadem" <[log in to unmask]>
Date:
Sun, 19 Apr 2009 19:22:41 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
John Goulet <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=utf-8
MIME-Version:
1.0
Parts/Attachments:
text/plain (79 lines)
Thanks, great info.I saved in my design note file. 
----- Original Message ----- 
From: "Richard D. Stadem" <[log in to unmask]> 
To: [log in to unmask] 
Sent: Thursday, March 19, 2009 10:37:18 AM GMT -05:00 US/Canada Eastern 
Subject: Re: [TN] Traces and vias under components 

Ok, I have finally seen enough emails on this subject to respond. 

First, many designs will not work with trace connections from chip cap 
and chip resistor pads going back under the component, because it 
essentially changes the rated capacitance or induces an RC network into 
the circuit. For certain high-speed RF circuits this is especially true. 

Second, soldermask is not defined as an insulator per IPC standards. 
Solder mask skips and discontinuities are allowed. Therefore the concern 
of entrapped flux under chip components creating a high-resistance or 
high-impedance short or path is very real, and has been documented many 
times. 

Third, the tented soldermask height is difficult for any PWB fabricator 
to control, and as such it quite often presents a little bump right 
between the pads. This leads to poor gasketing of the stencil during the 
printing process, which in turn leads to excess solder, bridging, solder 
balls, etc. Vias further away from the open apertures are isolated from 
the paste bricks, and are thus not an issue. 

For these reasons many companies adopted the design rule of no vias 
under or near chip pads, period. 
  

-----Original Message----- 
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete Houwen 
Sent: Thursday, March 19, 2009 8:13 AM 
To: [log in to unmask] 
Subject: Re: [TN] Traces and vias under components 

This is when it's good to be captive.  I get to make the dumb rules for 
myself! 

If that's what they want. that's what they get.  Say no, they'll find 
someone who will say yes.  And if it takes more layers to route, 
consider it an economic stimulus for the fab shops.  If the planes are 
so fragmented that they fail FCC or have SI problems, you'll get paid 
for a few more turns of the board. 

--------------------------------------------------- 
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
unsubscribe, send a message to [log in to unmask] with following text in 
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or 
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the 
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
archives of previous posts at: http://listserv.ipc.org/archives Please 
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815 
----------------------------------------------------- 

--------------------------------------------------- 
Technet Mail List provided as a service by IPC using LISTSERV 15.0 
To unsubscribe, send a message to [log in to unmask] with following text in 
the BODY (NOT the subject field): SIGNOFF Technet 
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) 
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest 
Search the archives of previous posts at: http://listserv.ipc.org/archives 
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 
----------------------------------------------------- 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2