TECHNET Archives

April 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
[log in to unmask], TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 14 Apr 2009 23:15:23 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; format=flowed; charset="iso-8859-1"; reply-type=original
From:
Parts/Attachments:
text/plain (83 lines)
You mean that such a bond degrades even if just being in constant room 
temperature and no power switching?
Inge


----- Original Message ----- 
From: <[log in to unmask]>
To: "TechNet E-Mail Forum" <[log in to unmask]>; "Inge" 
<[log in to unmask]>
Sent: Tuesday, April 14, 2009 11:07 PM
Subject: Re: [TN] Gold/Tin Intermetallics, why are we afraid?


> Hi Inge,
>
> Yes, the intermetallics itself is strong, BUT it doesn't count, as all 
> failures I've seen goes at the tin/intermetallics interface. The larger 
> were the platelets, the worse it looked.
>
> Regards,
>
> Vladimir
> ------Original Message------
> From: Inge
> Sender: TechNet
> To: [log in to unmask]
> ReplyTo: TechNet E-Mail Forum
> ReplyTo: Inge
> Sent: Apr 14, 2009 16:55
> Subject: [TN] Gold/Tin Intermetallics, why are we afraid?
>
> These infamous IMCs are like parias or ghosts in most people's mind in our
> business. I shocked our production guys recently by giving the advice to 
> let
> the boards go on. Large crystals and bad looking. But I always  try to 
> avoid
> exaggerations. If no serious temp changes are predicted, nor any severe
> power switching, why rework and risk introducing failures?  The actual
> components were very hard to rework, the cost had been unacceptable. I can
> see many of you get  the coffee wrong. I don't mean to spread quality
> distractions, I talk about very few boards and a unique situation. My
> statement was based on the fact that a gold tin intermetallic bond is
> extremly strong and can last long, if not exposed to what I pointed at
> earlier. I expect to be hammered down in the shop floor until only the 
> nose
> is visible....
>
> Inge
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
>
>
> SENTEC
> 11 Canadian Road, Unit 7.
> Scarborough, ON M1R 5G1
> Tel: (416) 899-1882
> Fax: (905) 882-8812
> www.sentec.ca
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2