Hi Amol!
Let me just say that I've never had to replace a stainless steel stencil
for anything other than it getting damaged (dented from something
getting dropped on it, etc.), or it becoming de-bonded from the
polyester mesh that holds it in the frame. With our new "frameless"
stencils I don't think I'll need to worry about that too much.
I have some stencils that I know we've built at least 5,000 - 8,000
boards with.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
Sent: Monday, April 13, 2009 12:09 PM
To: [log in to unmask]
Subject: [TN] Stencil Life
Dear Technetters,
Do anyone of you out there have a set value (time, # of prints etc.,)
that is used to replace a stencil with a new one?. I know "it depends"
on a large # of factors (stencil material, print speed, squeegee type,
print pressure, aperture size etc.), but is there some method to the
madness or is stencil replacement essentially a "as needed" item?
Thanks,
Amol
WARNING: Export Control
This document may contain technical data within the definition of the
International Traffic in Arms Regulations (ITAR), and subject to the
Export Control Laws of the U.S. Government. Transfer of such data by
any means to a foreign person, whether in the United States or abroad,
without proper export authorization or other approval from the U.S.
Department of State is prohibited.
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|