Brian and Blair,
From what I hear a sealed metal box will keep out water. A layer of steel
or glass does not allow water to pass.
Is this not the case for a "Thick" layer of silicone or epoxy?
What does "Thick" mean for different materials. How think does a silicone
adhesive need to be to equal the water penetration resistance of 1/16 (or
1/8) inch of steel?
How do folks measure how water (or even any ionic material) passes through
a substance?
Thanks,
Bob Kondner
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Blair Hogg
Sent: Thursday, March 05, 2009 8:38 AM
To: [log in to unmask]
Subject: Re: [TN] Comformal Coating vs Potting
Bob,
Most conformal coatings can and will pass moisture through to the assembly
in varying degrees, Thus, if there are any contaminants on the assembly
prior to coating that can activate with the addition of moisture the coating
will only slow down the effect. Also, if the environment in which your
module will be placed is humid for a significant portion of the time, it
will not have the opportunity to dry out, and its performance may be
affected.
Blair Hogg
On Wed, 4 Mar 2009 10:50:38 -0500, Robert Kondner
<[log in to unmask]> wrote:
>Hi,
>
> I have been playing with some conformal coating material and I have a
>couple of general questions.
>
>1. Coatings get VERY thin around sharp corners. Using a number of coats
>seems like the only way to build up any serious thickness.
>
>2. Potting seems like another name for "Very Thick Conformal Coating".
>
> I am looking as an application where a sensitive electronic module will be
>placed in a wet humid environment. It is a sensor going into the cooling
>tower of a HVAC system.
>
> After reading about conformal coating and playing with some sprays and
>brush on material I think thick potting is the only option to keep moisture
>out of circuits. We need at least 20 Meg ohm between circuits spaced 10
mils
>on FR4 material.
>
> Can anyone verify I am on the correct track and can they point me towards
>selecting the proper materials and process?
>
>Thanks,
>
>Bob Kondner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|