Craig,
Sorry for the late answer I have been traveling.
The first records were made of a lacquer acetate plasticized with castor
oil.
The next materials used were:
Shellac
Bakelite
Vinsol
Valtie
Vinyl chloride acetate
33-1/3 LP and 45rpm Record Material:
Vinyl records (33-1/3 LP and 45rpm) are made from polyvinyl chloride (PVC).
Information on record material types was taken in part from 'The Care and
Handling of Recorded Sound Materials' by Gilles St-Laurent Music Division of
the National Library of Canada, January 1996.
Vinyl chloride is a gas. PVC is a rigid solid and needs plasticizers to
make it less so. In the case of cable sheathing a lot of plasticizer is
needed and in many cases those plasticizers are the three phthalates on the
REACH SVHC list!
Bev
RIM
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Cullum
Sent: Thursday, March 12, 2009 5:11 PM
To: [log in to unmask]
Subject: [TN] Friday NTC question: is Vinyl really vinyl
Hi techxperts,
My mind got to wandering again, so here goes:
The contemporary term for what we called "records" (LP's and 45's) is
"vinyl".
But to me something that is vinyl would be a lot less rigid.
So, just what kind of material are records/"vinyl" made of?
Thanks in advance.
Craig Cullum, Engineering Technologist, AMTELCO
e: [log in to unmask]
[log in to unmask]
f: 608 838 8367
v: 608 838 4194, or 4197, x128
Please visit us at www.amtelco.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|