Hi Amol,
When you say: "we elected to just do a corner bond approach"--what exactly do you mean? after or before soldering?
If after soldering, that may have helped the corner SJs, but how did it help all the others?
Werner
-----Original Message-----
From: Rick Bell <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, 18 Mar 2009 4:50 pm
Subject: Re: [TN] Underfill Application
Amol,
I have some admittedly limited experience with underfilling CSP's for increased
reliability. Some answers to your questions:
1.) Our material selection initially was governed by a host of parameters--
reworkability (see next point), minimum dispense gap, process temperatures, cte
matching, filler content, etc. In my experience, trying to get a reworkable
version will greatly limit your choices.
2.) We used a Loctite material, I believe it was 3549. Please be aware that the
term "reworkable" is relative. We tried using it on polyimide flex substrates,
and found its reworkability was a matter of interpretation. Your mileage may
vary...
3.) We used an Asymtek dispense jet platform with very good results as far as
material deposition. Our only inspection capability was outsourced CSAM..
4.) Pitfalls-- Our biggest issues were some minor problems with adhesion to the
substrate/device, and incomplete encapsulation of a given solder joint due to
poor capillary fill on our device (this has highly detrimental effects in temp
cycle). My only advice there is that if you're going to attempt a full
encapsulation, have CSAM inspection available to verify your coverage, or some
very tight process controls once you have a benchmarked process.
In the end, we elected to just do a corner bond approach, rather than trying to
fully encapsulate the BGA array, and we had reasonable success in reliability
improvement.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
Sent: Wednesday, March 18, 2009 2:48 PM
To: [log in to unmask]
Subject: [TN] Underfill Application
Dear Technetters,
We are about the develop a process for underfilling BGAs for a high reliability
application. the underfill will be a rework able underfill. I wanted to poll the
technet on:
1. Guidance on material selection
2. most common materials being used out there and the process equipment
being used to do so.
3. Common pitfalls and things to lookout for
4. inspection techniques used to inspect the finished product
5. a good source for info on underfilling (books, papers etc.,)
Thanks in advance.
Regards,
Amol
WARNING: Export Control
This document may contain technical data within the definition of the
International Traffic in Arms Regulations (ITAR), and subject to the Export
Control Laws of the U.S. Government. Transfer of such data by any means to a
foreign person, whether in the United States or abroad, without proper export
authorization or other approval from the U.S. Department of State is
prohibited.
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|