TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Date:
Mon, 30 Mar 2009 14:04:18 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-15; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (123 lines)
I'm not sure that Vigon will be satisfactory for removing mineral oil 
residues and their additives, as these will not saponify in the amines. 
You will need something with the pH exceeding 12-13 and with stronger 
tensio-active components.

I'll shock you by suggesting a trichloroethylene blend in a 
zero-emissions cleaning machine with a vapour phase final. I don't care 
what people say, it is a damned good low-cost solvent, used sensibly it 
is perfectly safe, it is non-carcinogenic to humans (it is carcinogenic 
to rodents in high doses, but their metabolism of the substance is 
different) AND IT WORKS!!! (If needed, I have details of epidemiological 
studies with cohorts of tens of thousands supporting my statements.)

In the unlikely event that this alone would be insufficient for your 
needs, then consider an aqueous solution, depending on the residue 
analysis after TCE.

Brian

This alone would probably be sufficient and low-cost

Hernefjord Ingemar wrote:
> The tests will show. If one or two steps  can be left, of course very good. On the other hand, the cost for these units is so high, that some dollars saving is negligible. Unlike the normal production when cents are hunted for. 
> 
> The alcaline bath will possibly be superseded by our Vigon 200 tunnel cleaner. 
> /Inge 
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak
> Sent: måndag 30 mars 2009 11:28
> To: [log in to unmask]
> Subject: Re: [TN] Titanium
> 
> Ingmar:
> The process you suggest probably will work, but I suspect it is overkill.  I suspect that the alkaline cleaner will be enough on its own.
> 
> Good luck.
> Rudy Sedlak
> 
> --- On Sun, 3/29/09, Hernefjord Ingemar <[log in to unmask]> wrote:
> 
> From: Hernefjord Ingemar <[log in to unmask]>
> Subject: Re: [TN] Titanium
> To: [log in to unmask]
> Date: Sunday, March 29, 2009, 11:58 PM
> 
> Thank you, Rudy&Steve.
> 
> It seems as a suitable treatment would be this one:
> a)Solvent degrease, followed by
> b)Alcaline bath, followed by
> c)DI ultrasonic bath, followed by
> d)Micropowder blast, followed by
> e)HNO3 dip, followed by
> f)DI ultrasonic bath.
> 
> We will try this today already. We do not like HF, so that kind of process is skipped. Our problem is not primarily to remove the oxide, but to ascertain that all threading/cutting oil is gone, also that the numerous micro pores are emptied from their content.
> 
> /Inge
> 
> 
>  
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of R Sedlak
> Sent: lördag 28 mars 2009 20:19
> To: [log in to unmask]
> Subject: Re: [TN] Titanium
> 
> Although Titanium lightly alloyed is used in some joint replacements, it may well be more commonly known for its use as Nitinol, a Nickel/Titanium alloy, which has weird "memory" properties.  Nitinol is one of the more common stent materials.
> 
> Cleaning Titanium is quite difficult, particularly if it is heavily oxidized, as the common "cleaning" agent, (Hydrofluoric Acid) attacks Titanium vigorously, and then to frost the cake, this causes Hydrogen embrittlement.
> 
> Not everyone/everywhere is as "enlightened" as we like to think we are, and yes, there is still choro-ethanes still in use in cleaning (Think "dry cleaning" clothes).
> 
> There are proprietary cleaners which purport to get around these issues.   If interested, contact me off Technet.
> 
> Rudy Sedlak
> RD Chemical Company
> 
> 
> 
> 
> 
>       
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> 
> 
>       
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2