Ingemar,
Check out Product Finishing [magazine] On-Line to see if you can find some
additional insight http://www.pfonline.com/
http://www.pfonline.com/clinics/ - list of clinics they offer
Try e-mailing the guy in the cleaning clinic -
http://www.pfonline.com/clean/clinics.html
An article I found when searching for "medical titanium" in their past
articles http://www.pfonline.com/articles/web110101.html - this article
indicates the user is using in 1,1,1 trichloroethylene. Wonder how old the
article actually is?
From the cleaning clinic - "cleaning titanium"
http://www.pfonline.com/articles/clinics/1206cl_clean3.html
http://www.pfonline.com/articles/clinics/0808cl_clean4.html
I'll ask my pacemaker buds to see if they have a quick answer that can be
shared.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Inge
Sent: Friday, March 27, 2009 3:02 PM
To: [log in to unmask]
Subject: [TN] Titanium
Hi all,
this is little odd question in this forum, but I try:
after machining a complex structure in pure Titanium, how do you clean the
part to a medical cleanliness level?
Threading/cutting oil was a mineral oil with added Sulphur and Zinc /MSDS
7047. I have an idea about alcaline cleaning with
ultrasonic followed by etching in a 10% water/HNO3 solution, ended with
ultrasonic water washing in distilled water.
Anyone with experience?
/Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|