TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Date:
Fri, 13 Mar 2009 16:53:27 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-15; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (177 lines)
Well, I may be 76, but I remember, as a 12 y-o boy, in our first-year 
chemistry class, putting some potassium nitrate in a test tube and 
heating it. A glowing wood splint introduced in the tube suddenly burst 
into flames. Now I wonder where that oxygen came from that caused this? 
Maybe inorganic chemistry has changed its rules in the intervening 64 
years??? :-)

Brian

R Sedlak wrote:
> This is the reverse of my experience.   I am used to Nitrites oxidizing to Nitrates, not vice versa.   And to produce Nitrides in the presence of air I suspect might take extraspiritual influence.
> 
> Rudy Sedlak
> RD Chemical.
> 
> 
> --- On Fri, 3/13/09, Brian Ellis <[log in to unmask]> wrote:
> From: Brian Ellis <[log in to unmask]>
> Subject: Re: [TN] Bath Salts
> To: [log in to unmask]
> Date: Friday, March 13, 2009, 12:31 AM
> 
> With such oxidising substances at 300°C, the excitement would not be
> long in coming. :-) I suggest adding some charcoal and sulfur to the mix
> while you're about it! :-D Incidentally, the nitrates would become
> nitrites and then nitrides in time, so the mix wouldn't be stable, anyway!
> 
> Brian
> 
> John Maxwell wrote:
>> Rudy,
>> I always enjoyed watching chemical reactions in an exciting way at a safe
> distance when I was in the Air Force. Some were 1000# gravity bombs and those
> required a rather large safe viewing distance.
>> John Maxwell
>> ----- Original Message ----- From: "R Sedlak"
> <[log in to unmask]>
>> To: <[log in to unmask]>
>> Sent: Thursday, March 12, 2009 3:13 PM
>> Subject: Re: [TN] Bath Salts
>>
>>
>>> Chris:
>>> The exact formula is not critical, do not sweat it, pick mid values
> and go with it.
>>> BUT, do realize this stuff is NOT mother's milk, and in fact,
> could corrode virtually any metal except 300 series stainless steel, and will
> react, perhaps in an "exciting way", with organics spilled into the
> bath.
>>> The big advantage of the Dow Corning stuff it is so benign, and
> won't corrode, or react in exciting ways.
>>> Rudy Sedlak
>>>
>>> --- On Thu, 3/12/09, Chris Mahanna <[log in to unmask]> wrote:
>>> From: Chris Mahanna <[log in to unmask]>
>>> Subject: [TN] Bath Salts
>>> To: [log in to unmask]
>>> Date: Thursday, March 12, 2009, 1:20 PM
>>>
>>> Hello all,
>>>
>>> Does anyone know if there is extra fairy dust in bath salts (other
> than
>>> anticake and pink food coloring)?  For that matter, what's
> anticake?
>>> I need to run liquid thermal shock testing at 300C.  We've been
> using Dow
>>> Corning 710.  In an open system, kinda cost prohibitive.
>>>
>>> I gather from MSDSs that we can mix a eutectic somewhere around:
>>>
>>> Potassium Nitrate: 40-50%
>>> Sodium Nitrate: 10-20%
>>> Sodium Nitrite: 30-40%
>>>
>>> Extra credit to any mixing experts that know the exact formula for
> ~200-350C.
>>> I can source the salts a couple blocks away for $, or the mix from
> across the
>>> country for $$$$$.
>>> I'd much prefer going down the street.
>>>
>>> Thanks!
>>>
>>> Chris
>>>
>>> ---------------------------------------------------
>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>> To unsubscribe, send a message to [log in to unmask] with following
> textin
>>> the BODY (NOT the subject field): SIGNOFF Technet
>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>> To receive ONE mailing per day of all the posts: send e-mail to
>>> [log in to unmask]: SET Technet Digest
>>> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
>>> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
>>> additional information, or contact Keach Sasamori at [log in to unmask] or
>>> 847-615-7100 ext.2815
>>> -----------------------------------------------------
>>>
>>>
>>>
>>>
>>> ---------------------------------------------------
>>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>>> To unsubscribe, send a message to [log in to unmask] with following
> textin
>>> the BODY (NOT the subject field): SIGNOFF Technet
>>> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>>> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
>>> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
>>> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or
> contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>>> -----------------------------------------------------
>>>
>>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: http://listserv.ipc.org/archives
>> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> 
> 
>       
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2