TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Sat, 7 Mar 2009 09:49:02 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner engelmaier <[log in to unmask]>
Subject:
From:
Werner engelmaier <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
<EC1BA3606CFD45768A2C512CF4FAF774@ingemar63eaed8>
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (186 lines)
 Hi Amol,
Unfortunately, in most cases nobody analyzes failures. The reason is that to do a proper root cause analysis takes time, resources and expertize—and in many cases is too late for corrective action.
This is too bad, because a lot could be learned for future designs.
There are 2 important aspects to failure analysis—the physics-of-failure aspect and the statistical failure information.
Failures occur for the main part for 3 reasons: 1) inadequate design, allowing premature wear-out and/or overstress conditions, 2) insufficient quality, due to bad processing and causing latent defects, and 3) misuse.
Commercial or in-house laboratories can be utilized to establish failure modes and compliance with standards/specifications, however, the determination of the failure root cause typically requires an expert.

Werner


 


 

-----Original Message-----
From: Inge <[log in to unmask]>
To: [log in to unmask]
Sent: Sat, 7 Mar 2009 5:23 am
Subject: Re: [TN] Failure Data Analysis Techniques









We follow HDB-217 and 883 and 1553 stds in essential. One NASA example: 
 

http://www.moasoftware.co.kr/board2/data/design/dfr07.pdf 
 

Another typical example is this good one from EXIDA: 
 

http://www.prelectronics.com/filer/9202_FMEDA.pdf 
 

However, the handbook refer to one decade or more old statistics, so for 
many new components derating and failure rate figures etc are not available. 
You have to make your own FMEA, Arrhenius nomograms and all that stuff. 
 

I'm not 
an expert but have been involved frequently in the field. We had 
several people with a PhD degree working with Failure Data Analysis, but 
nowadays only one guy is left. The reason is that the reliability of many 
processes has been improved a lot. One or two decades ago, we had boxes with 
hundreds of components waiting for registering and analysis. Today nearly 
nothing. If there are any issues, we are causing them ourselves in the 
manufacturing process. And even these are few nowadays. Those of you who 
have been involved, remember all the problems with tantalum caps? Or CMOS? 
Or humidity in DIPs? Ahora nada de estos. 
 

Best you can do to get answer on your questions is to call someone at NASA 
(e.g. Mr Brusse, who use to read TN mails). Or ESTEC. Or Vernier Anglemajor. 
 

Inge 
 


----- Original Message ----- 
From: "Kane, Amol (349)" <[log in to unmask]> 

To: <[log in to unmask]> 

Sent: Friday, March 06, 2009 3:48 PM 

Subject: [TN] Failure Data Analysis Techniques 
 


Dear Technetters, 

I am doing some research (for my PhD dissertation) on the common Failure 
Data Analysis Techniques (or software) people are using in the industry to 
analyze their failure data. Specifically, end of line SMT defects across all 
assemblies and product lines. I realize that failure data is something that 
all companies will not discuss. I am not looking for results, just methods 
that you might be using to arrive at informed conclusions.
 Any responses 
(offline or on the forum) will be greatly appreciated 
 

Regards, 

Amol 
 

 

WARNING:  Export Control 

This document may contain technical data within the definition of the 

International Traffic in Arms Regulations (ITAR), and subject to the Export 

Control Laws of the U.S. Government.  Transfer of such data by any means to 
a 

foreign person, whether in the United States or abroad, without proper 
export 

authorization or other approval from the U.S. Department of State is 

prohibited. 
 

CONFIDENTIALITY NOTICE: 

This e-mail, and any attachments, is for the sole use of the intended 

recipient(s) and may contain information that is confidential and 

protected from disclosure under the law. Any unauthorized review, use, 

disclosure, or distribution is prohibited. If you are not the intended 

recipient, please contact the sender by reply e-mail, and delete/destroy 

all copies of the original message and attachments. 

Thank you. 
 

--------------------------------------------------- 

Technet Mail List provided as a service by IPC using LISTSERV 15.0 

To unsubscribe, send a message to [log in to unmask] with following text in 

the BODY (NOT the subject field): SIGNOFF Technet 

To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL) 

To receive ONE mailing per day of all the posts: send e-mail to 
Listserv@ip
c.org: SET Technet Digest 

Search the archives of previous posts at: http://listserv.ipc.org/archives 

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815 

-----------------------------------------------------  

--------------------------------------------------- 

Technet Mail List provided as a service by IPC using LISTSERV 15.0 

To unsubscribe, send a message to [log in to unmask] with following text in 

the BODY (NOT the subject field): SIGNOFF Technet 

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) 

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest 

Search the archives of previous posts at: http://listserv.ipc.org/archives 

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815 

----------------------------------------------------- 



 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2