I am sorry but I don't see the pictures. Not understanding the complete
stack up of your flex but it sounds like you are having a lot of movement
during the vendors processing of the manufacturing panel which in turn gives
the assembly process a headache.
- Small pallets are best when processing type 3 circuits
- You can ask your flex vendor to give you the offsets they used @ drill or
final layer image and use these for your paste stencil.
- I have seen the gold wash between metal and actually stick to the
pre-cured adhesive that is sometimes left behind after etch if using a LF9
type of material. This only happen when we had mass exposed areas like fine
pitch components.
Please update your contact for Jim Mahoney
[log in to unmask]
Thank you,
Jim Mahoney
Quick Turn Flex Circuits, LLC
Applications Project Manager
P# 603-821-6571
F# 603-821-5723
M# 603-305-6250
** This email and all attachments have been scanned prior to being sent**
Confidentiality Notice: This page and any accompanying documents contain
information that is confidential, privileged or exempt from disclosure and
is intended for the exclusive use of the addressee. If you are not the
intended recipient, you are hereby notified that any disclosure, copying,
distribution or use of the contents of this information in any manner is
strictly prohibited.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dave Connitt
Sent: Thursday, March 05, 2009 3:09 PM
To: [log in to unmask]
Subject: [TN] ENIG Question
Hello All,
I have a question regarding a strange situation regarding reflow
soldering ENIG finish boards.
We have seen a few boards that have what seems to be gold "washing "
down between pads and creating shorts. This seems to come and go. This
is a flex circuit that is placed on a pallet to go through our SMT line.
One other bothersome issue is that we are having difficulty getting
proper solder stencil alignment across all the flexes in the pallet. I
am pushing to have the flex "panelized" from the vendor to increase
positional accuracy but the jury is still out on that.
I suspect these two issues are related. If the solder gets deposited
"off pad"slightly could the washing process be moving some of the gold
in between pads? I attached an example.
Has anybody come across this?
If so, what was the solution?
Thanks,
Dave Connitt CID+
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|