Juan,
To qualify a cleaning process, depending on your requirements, I would suggest:
1. Visual cleanliness
2. Ionic contamination levels (Ionograph, omegameter, or equivalent)
3. Ion Chromatography - to determine the types of ionic contamination and their levels.
While there is no formal guide to certify a cleanliness process, these are the types of tests I used to qualify my processes in an aerospace environment.
I echo Joe's sentiments about checking the equipment and chemistry. I would also check for material compatibility. Some cleaning chemistries are more aggressive than others and could pose a danger to specific components and materials.
Hope this helps.
Good Luck.
Lee Whiteman, PMP
Senior Member Engineering Staff
L-3 Communications East
Telephone: (856) 338-3508
FAX: (856) 338-2906
E-Mail: [log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Juan T. Marugán
Sent: Thursday, March 05, 2009 10:45 AM
To: [log in to unmask]
Subject: [TN] Cleaning equipment validation.
Hi,
We are going to change our cleaning equipment and I would like to know if
there is a guide -or what tests can be carried out- to validate a new cleaning
equipment.
We are using rosin fluxes for Class 3 products.
Thank you in advance for your help.
Juan T. Marugán
Indra Sistemas SA
Spain
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|