TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 30 Mar 2009 20:01:18 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Werner Engelmaier /* <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
<EA0AC47D7E5C41BE942E67BA3CE1C3B4@ingemar63eaed8>
Content-Transfer-Encoding:
7bit
MIME-Version:
1.0
Parts/Attachments:
text/plain (188 lines)
 Hi Inge,
You are going super-conservative in your old age. Heck, I have had accelerated tests with mean cyclic lives of 100 cycles and others with no failures in 100,000 cycle---It all depends.
If you understand the load drivers and the connections to cyclic life, you can execute a proper Design-for-Reliability in almost all cases; the tricky part is getting all the necessary info, AND getting correct info.

Werner


 


 

-----Original Message-----
From: Inge <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, 30 Mar 2009 6:28 pm
Subject: Re: [TN] solder fatigue predictions for highly asymmetrical duty cycles









not an answer, but some reflections....?
?

I'm not a guru, more of a practical gnu. We have some math specialists who 
have produced models and calculations that make a normal reader exhausted to 
go from page 1 to page 200. After going through some reports like that, you 
feel rather disoriented. So, in order to know about the failure modes and 
six sigma, Time to Failure and such parameters, we decided to go the 
hands-on way. We 'simply' produced a lot of cloned boards with a substantial 
lot of components on, and started temp cycling with various symmetries and 
limits. Believe it or not, we have passed 10,000 cycles in some cases. The 
result will not be known until the end of this year. This method is not very 
comfortable either, making all these hundreds of microscope inspections and 
measure daisy chains and other stuff. Because our customer wants this way, 
we simply do it. Personally, I prefer neither of the ways, but more of a 
cautious and well performed design.  Follow the derating rules, don't buy 
components from unknown manufacturers,  hold back when the design engineers 
excess in very large or very odd boards,  keep to a board producer you know, 
don't mix extremly hot components with mW components and a lot more of 
goodies .  Sounds like stopping the development of new technology, but after 
reading Toyota's LEAN thinking, it seems as making many small development 
steps are safer, than to make a brand new super design. In earlier days, we 
had time to make prototypes, take our time and make a small pre-series, then 
introduce improvements, longlife test and slowly start series production. 
Now we go directly from CAD engineering to production....?

says an old dog?
?

Inge?
?


----- Original Message ----- 
From: "Nieznanski, John A - SSD" <[log in to unmask]>?

To: <[log in to unmask]>?

Sent: Monday, March 30, 2009 10:05 PM?

Subject: [TN] solder fatigue predictions for highly asymmetrical duty cycles?
?


Hello Tech-Net Gurus,?
?

The solder fatigue parameters called out in IPC-D-279, IPC-SM-785 and 
IPC-9701 all assume symmetrical (i.e. 50%) duty cycles and temperature 
swings. This raises the question as to how far these calculations can be 
pushed to predict solder fatigue in low duty cycle, variable duty cycle or 
high duty cycle applications.?
?

In particular, Tsj ( = mean cyclic solder joint temperature), and tD ( = 
half-cycle dwell time in minutes) are both used and are directly affected by 
duty cycle. It is simple enough to recalculate these values based on 
asymmetrical duty cycles, but how do we know that the predicted solder 
fatigue results are still valid? If we know, do we know what assumptions are 
required to make the results valid? This seems like a fairly common 
situation. Has anyone correlated measured results to predictions in this 
regard??
?

Specifically, there are numerous caveats in the specs including for example, 
high-frequency (e.g, vibration) conditions where tD < 1 second, but none of 
these caveats apply here.?
?

For example, with a power on dwell time of 6 minutes (system reaches thermal 
equilibrium in < 1 minute) and a power off dwell time of 54 minutes (10% 
duty cycle), I assume I can simply use tD = 6 minute dwells and Tsj = 
average solder joint temperature over 60 minute cycle. Do you agree with 
this approach??
?

Another potential case of interest is if the duty cycle is reduced to 
something less than 1 minute (but more than 1 second; not a vibration 
situation), such that the stabilized operating temperature is not reached. 
Can any valid fatigue calculations be performed in these cases if I can 
determine a valid Tsj for a 1 minute tD??
?

Thanks in advance for your insights and assistance.?
?

Best regards,?
?

John N.?
?


________________________________?

This e-mail and any files transmitted with it may be proprietary and are 
intended solely for the use of the individual or entity to whom they are 
addressed. If you have received this e-mail in error please notify the 
sender.?

Please note that any views or opinions presented in this e-mail are solely 
those of the author and do not necessarily represent those of ITT 
Corporation. The recipient should check this e-mail and any attachments for 
the presence of viruses. ITT accepts no liability for any damage caused by 
any virus transmitted by this e-mail.?
?

---------------------------------------------------?

Technet Mail List provided as a service by IPC using LISTSERV 15.0?

To unsubscribe, send a message to [log in to unmask] with following text in?

the BODY (NOT the subject field): SIGNOFF Technet?

To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)?

To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest?

Search the archives of previous posts at: http://listserv.ipc.org/archives?

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815?

----------------------------------------------------- ?

---------------------------------------------------?

Technet Mail List provided as a service by IPC using LISTSERV 15.0?

To unsubscribe, send a message to [log in to unmask] with following text in?

the BODY (NOT the subject field): SIGNOFF Technet?

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)?

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest?

Search the archives of previous posts at: http://listserv.ipc.org/archives?

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815?

-----------------------------------------------------?



 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2