TECHNET Archives

March 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Sat, 28 Mar 2009 23:18:18 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, SUBSCRIBE technet legg <[log in to unmask]>
Subject:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="ISO-8859-1"
From:
SUBSCRIBE technet legg <[log in to unmask]>
Parts/Attachments:
text/plain (107 lines)
A little late for this thread, but outgassing plasticizers from PVC can
attack other plastics. 

As an example, the insulating handles on a pair of wire nippers recently
dissolved large pits in the transparent face of a stop-watch, in one of my
tool kits. The points of near-contact retain their newly acquired flow
characteristic. Tacky. 

The nippers are US-origin Xuron trade mark, so please don't start flaming
off-shore sources. The insulation on the handles is splitting, without any
regular use.

RL

On Wed, 18 Mar 2009 21:34:42 -0400, Bev Christian
<[log in to unmask]> wrote:

>Craig,
>Sorry for the late answer I have been traveling.
>
>The first records were made of a lacquer acetate plasticized with castor
>oil.
>The next materials used were:
>Shellac
>Bakelite
>Vinsol
>Valtie
>Vinyl chloride acetate
>
>33-1/3 LP and 45rpm Record Material:
>Vinyl records (33-1/3 LP and 45rpm) are made from polyvinyl chloride (PVC).
>
>Information on record material types was taken in part from 'The Care and
>Handling of Recorded Sound Materials' by Gilles St-Laurent Music Division of
>the National Library of Canada, January 1996.
>
>Vinyl chloride is a gas.  PVC is a rigid solid and needs plasticizers to
>make it less so.  In the case of cable sheathing a lot of plasticizer is
>needed and in many cases those plasticizers are the three phthalates on the
>REACH SVHC list!
>Bev
>RIM
>
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Craig Cullum
>Sent: Thursday, March 12, 2009 5:11 PM
>To: [log in to unmask]
>Subject: [TN] Friday NTC question: is Vinyl really vinyl
>
>Hi techxperts,
>My mind got to wandering again, so here goes:
>
>The contemporary term for what we called "records" (LP's and 45's) is
>"vinyl".
>But to me something that is vinyl would be a lot less rigid.
>
>So, just what kind of material are records/"vinyl" made of?
>
>Thanks in advance.
>
>Craig Cullum, Engineering Technologist, AMTELCO
>e: [log in to unmask]
>   [log in to unmask]
>f: 608 838 8367
>v: 608 838 4194, or 4197, x128
>
>Please visit us at www.amtelco.com
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2