Joe Macko
你好!
回流焊接的熔融区的温度应适当地提高,建议实际最高温度在230℃±5℃。
陈昆
2009-3-2
-----邮件原件-----
发件人: TechNet [mailto:[log in to unmask]] 代表 Joe Macko
发送时间: 2009年2月28日 星期六 0:04
收件人: [log in to unmask]
主题: [TN] Reflowing CBGA component (with high Sn balls) using Eutectic solder paste
Hi All,
My question is related to the soldering of IBM PPC CBGAs type components
(that have Sn90Pb10 solder balls) using Sn63 paste onto ENIG finished
boards. What are the "determining-factors" to improve the
wetting/diffusion of the eutectic solder paste into the high Sn solder
balls. The eutectic solder appears to wet well to the ENIG pads located
on the board but occasionally I see eutectic solder fillets that do not
always appear to fuse well with the high Sn content balls (if fuse is
the correct word?). thx
Best Regards,
-Joe
"This e-mail and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as U.S. Government export controlled technical data. If you are an unintended recipient of this e-mail, use, disclosure or distribution of its content is prohibited. Please notify the sender by return e-mail and immediately delete this message."
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|