Hey Kevin,
No doubt finger prints can be catastrophic in some situations. But I think you would be best served to disconnect your post cc aesthetics from the science.
ROSE testing would be cheap and dramatic. Customer refusing part is dramatic.
IMO you've got two choices 1) listen to your customer and sell no fingerprints, or 2) run J-STD-001 SIR/ECM on A-36s or B-52s and show that it (maybe) doesn't matter after coat.
Is handling the assemblies from the edges not a workable solution?
Chris
Chris Mahanna
Robisan Laboratory Inc.
6502 E 21st Street
Indianapolis, Indiana 46219
317.353.6249
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kevin Glidden
Sent: Wednesday, March 04, 2009 8:27 AM
To: [log in to unmask]
Subject: [TN] Gloved Hands / Fingerprints / Failure Articles
Hello everyone,
We are in the midst of a proposal from myself and manufacturing engineering to require use of gloves or finger cots throughout our PCB assembly process.
We had considered that it really would only be required after final cleaning, but for uniformity would require it all steps including population. We have of course met with a real resistance, particularly from the final assemblers who are stating it doesn't matter once the conformal coat is on. I can see at least some logic in that, and admittedly a large portion of our argument is aesthetics (we don't want fingerprints on the boards even after coating), but it would be really nice to have some sort of scare tactic, like an article or something that related a PCB failure to fingerprints or handling contamination. Anyone have such a thing?
Thanks!
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|